Dow
Dow Silicone Electronics Protection, Thermal Management and Liquid Cooling Solutions
Dow supplies silicone-based materials for bonding and sealing, electronics protection, thermal management, conformal coating, encapsulation, and liquid cooling. Krayden-relevant technologies include DOWSIL™ adhesive sealants, primers, thermal interface materials, conformal coatings, and silicone foams; SYLGARD™ dielectric gels and elastomer systems; DOWFROST™ inhibited heat-transfer fluids; and selected XIAMETER™ silicone materials for industrial processing and formulation applications.
As an authorized Dow distributor, Krayden supplies a broad selection of Dow materials and provides technical guidance for product selection, application requirements, processing considerations, and comparison of candidate materials. Cure behavior, substrate compatibility, bond-line or gap geometry, dispensing method, electrical requirements, thermal performance, and fluid-system compatibility are product- and application-specific and should be confirmed for the selected formulation and assembly.
Markets Served by Dow
Featured Dow Brands
Four Dow brands represented across silicone bonding, electronics protection, thermal management, heat-transfer fluids, and industrial silicone materials.
DOWSIL™
Silicone adhesives, sealants, conformal coatings, encapsulants, thermal materials, foams, primers, and related electronics and industrial materials.
SYLGARD™
Silicone dielectric gels and elastomer systems used for potting, encapsulation, casting, cushioning, and low-stress electronics protection.
DOWFROST™
Inhibited heat-transfer fluids used in industrial cooling, closed-loop systems, and appropriate data-center and liquid-cooling applications.
XIAMETER™
Silicone fluids, elastomers, intermediates, and related materials used in industrial processing and formulation applications.
Adhesives & Sealants
Dow bonding and sealing materials include one-part RTV silicone adhesive sealants, higher-performance silicone adhesive technologies, and primers or adhesion promoters used to prepare challenging substrates. Selection depends on cure method, handling strength, substrate combination, bond-line or seal geometry, environmental exposure, production method, and whether primer-assisted adhesion is required for the specified assembly.
Encapsulants & Gels
Dow dielectric gels and silicone elastomer systems protect electronic assemblies through low-stress cushioning, dielectric protection, potting, casting, and environmental isolation. Soft gels are suited to sensitive components where mechanical stress must be limited, while cured elastomer systems provide more defined support and encapsulation. Selection should account for cured modulus, working time, cure schedule, fill geometry, component sensitivity, dielectric requirements, and rework strategy.
Thermal Interface Materials
Dow thermal-management materials span curable gap fillers and thermal gels, thermally conductive adhesives, non-curing compounds and greases, and thermally conductive encapsulants. Selection should start with the required thermal path and gap or bond-line thickness, then account for compressibility, dispensing method, cure requirements, electrical insulation, mechanical attachment, reworkability, component stress, and service conditions.
Conformal Coatings
DOWSIL conformal coatings protect printed circuit assemblies from moisture, contamination, corrosion, and environmental exposure using multiple processing approaches. Depending on the product, options include moisture cure with room-temperature or heat-accelerated processing, UV cure with secondary moisture cure, lower-VOC solvent-borne systems, and no-added-solvent technologies. Selection should consider application method, cure window, coating coverage, production-line compatibility, rework needs, and required assembly protection.
Liquid Cooling & Heat Transfer Fluids
Dow supports liquid-cooling architectures from direct-to-chip technology cooling loops to facility water-loop heat transfer and immersion cooling. DOWFROST LC-25 is positioned for direct-to-chip data-center cooling, while other DOWFROST fluids serve closed-loop infrastructure and DOWSIL dielectric fluids support immersion-cooling designs. Fluid selection is system-specific and should account for loop materials, heat load, corrosion control, operating temperature, electrical requirements, maintenance practices, and equipment-manufacturer guidance.
Silicone Foams & Gasketing
DOWSIL two-part silicone foams can be dispensed and cured directly on parts to create integrated compression gaskets and environmental seals. These materials are relevant to automotive components, electrical housings, exterior lighting, appliances, and industrial enclosures where sealing force, gap variation, compression recovery, vibration damping, and automated gasket placement are important selection factors.
Talk to our Experts
Whether you are comparing Dow materials for bonding and sealing, electronics protection, conformal coating, thermal management, gasketing, or liquid cooling, Krayden can help evaluate product fit, application requirements, process constraints, and candidate materials for your assembly or cooling system.
Dow Quick Reference
251 products
-
DOWFROST LC 25 Heat Transfer Liquid
- Made with Dow PURAGUARD™ USP/EP grade PG (>99.8% purity)
- Freeze protection to –10°C (14°F)
- Formulated for high-efficiency heat transfer
-
DOWSIL™ 1-2577 Conformal Coating
- One-part silicone conformal coating
- UV indicator for inspection and quality control
- High dielectric strength and electrical insulation
-
-
DOWSIL™ 7091 Adhesive Sealant
- Non-sag rheology
- One-part moisture cure
- Stable and flexible from -40 to 180℃
-
DOWSIL™ EE-3200 Low Stress Silicone Encapsulant
- Low viscosity for flow into small gaps and complex PCB assembly spaces
- Soft, low-stress encapsulation during thermal cycling
- UL 94 V-0 and UL RTI rated at 150°C
-
DOWSIL™ TC-2035 CV Thermally Conductive Adhesive
- 3.3 W/m·K thermal conductivity
- Ultra-thin bondline thickness
- Low volatile content
-
DOWSIL 3-4154 Dielectric Gel Kit
- Electrically Insulating Material
- 550 mPa s Mixed Viscosity
- 180-Minute 80 deg C Cure
-
DOWSIL 550 SILICONE FLUID
- Silicone Fluid Formulation
- High-Temperature Silicone-Fluid Stability
- Low-Volatility Silicone Fluid
-
DOWSIL 93-104 Ablative Material Kit
- Protects surfaces from direct flame and extreme heat exposure
- Forms a tough char with less than 0.1 mm/s penetration
- Supports brush, roll, trowel, or molded application methods
-
DowSil 3-6077 RTV Silicone Ablative
- 0.035 mm/s Ablation Penetration Rate
- 2 to 3-Hour Working Window
- Spray or Trowel Application
-
Dow XIAMETER PMX 200
- 1,000 cSt Polydimethylsiloxane Fluid
- Surface Tension of 21.2 dynes/cm
- Dielectric Strength of 400 volts/mil
-
DOWSIL 20
- Heat-Stable Non-Carbonizing Parting Film
- Solvent-Dilutable Release Formulation
- Plastic/Adhesive/Elastomer Product Applications
-
DOWSIL 3-6548
- Fire-Resistant RTV Silicone Foam
- 2x to 4x Liquid-Volume Expansion
- Flexible Medium-Density Ozone/UV-Resistant Foam
-
DOWSIL 3-6559
- Adjustable 1 to 5 Wt% Addition Level
- 4 to 12-Hour Cure Window
- Surface/Environment Cure-Inhibition Management
-
DOWSIL 510
- Available in Four Viscosities
- High-Temperature Fluid Stability
- Low-Volatility Process Fluid
-
DOWSIL 710
- Up to 260 deg C Closed-System Service
- Low-Volatility Oxidation-Resistant Fluid
- High-Temperature Lubrication/Heat-Transfer Applications
-
DOWSIL DS-2025
- Cured Silicone Residue Removal
- Up to 400 g/L Silicone Solubilization
- Below 10 cP Low Viscosity
-
DOWSIL EC-6601
- 86 dB 1 kHz to 8.5 GHz Shielding
- 2.7E-3 ohm-cm Volume Resistivity
- One-Part Room-Temperature Moisture Cure
-
-
DOWSIL FS1265
- 100% Active Fluorosilicone Foam Control
- Chlorinated-Solvent-Insoluble Foam-Control Formulation
- 300/1,000/10,000 mm^2/s Viscosity Grades
-
DOWSIL OS-125
- Silicone-Contamination Cleaning Solvent Blend
- Immersion, Spray, Rinse, or Wipe Cleaning
- ppm-Level Residual Silicone
-
DOWSIL OS-20
- Immersion, Spray, or Wipe Cleaning
- Very-Low-Residue Complete Evaporation
- 0 g/L US VOC-Exempt Solvent
-
DOWSIL Q2-1346
- Low Sodium and Potassium Impurity Limits
- Clear Liquid Supplied Free from Suspended Matter
- Long 900-Day Shelf Life
-
-
DOW XR-1541
- E-Beam Patternable, Negative Tone
- Etch Resistance Surface Treatment
- High Purity Surface Treatment
-
DOWSIL 520
- Water-Dilutable 40% Active Emulsion
- Deep Mineral-Substrate Penetration
- Substrate-Specific Water Repellency
-
-
DOWSIL EC-8425
- Below 0.01 ohm cm Resistivity
- Low-Temperature Conductive Adhesive Cure
- Greater Than 20% Elongation
-
-
-
DOWSIL HV496
- Elastomeric Textile Finishing
- Leather Top-Finish Dilution Stability
- Water-Repellent Mineral-Wool Treatment
-
-
DOWSIL™ 1-2620 Low VOC Conformal Coating
- One-part silicone conformal coating
- Wide operating temperature range (-45°C to 200°C)
- UV indicator for inspection and process control
-
DOWSIL™ 3-4207 Dielectric Tough Gel Kit
- Multiple cure schedule for flexible processing.
- Translucent green with UV indicator support for automated inspection.
- 59 Shore 00 toughened gel with UL 94 V-1 and EN 45545-2 R25 HL3 listed
-
-
DOWSIL™ Q1-9226 Thermally Conductive Adhesive
- Two-part system
- Accelerated heat cure
- Robust mechanical & electrical profile
-
DOWSIL™ 3140 RTV Coating
- One-part silicone coating for room-temperature curing
- Resistant to moisture, chemicals, and UV
- Low viscosity for uniform coating and complete coverage
-
DOWSIL™ 3-4150 Dielectric Gel Kit
- Low viscosity and room temperature cure gel
- Low stress
- Excellent dielectric performance
-
DOWSIL™ EI-2888 Primerless Silicone Encapsulant Kit
- Primerless processing for simpler assembly workflows
- Optically clear protection for LED and display electronics
- Soft silicone encapsulation for environmental and electrical protection
-
DOWSIL™ TC-2022 Thermally Conductive Adhesive
- Heat curable at moderate temperatures
- Cost effective with rapid/low temperature cure
- Applicable on heat-sensitive substrates and components
-
DOWSIL 3-0115 Automotive Sealant
- Automotive Powertrain-Fluid Resistance
- Blowout-Resistant In-Line Leak Testing
- Primerless Metal and Plastic Adhesion
-
DOWSIL™ 3-1944 RTV Coating
- One-part silicone coating, room-temperature curing
- Low viscosity for complete wetting of complex geometries
- Durable, flexible protective layer
-
DOWSIL™ EI-2888 Primerless Silicone Encapsulant Kit
- Primerless processing for simpler assembly workflows
- Optically clear protection for LED and display electronics
- Soft silicone encapsulation for environmental and electrical protection
-
DOWSIL™ TC-5026 Thermally Conductive Compound
- Ultra-thin bondline capability of approximately 0.007 mm
- Suitable for CPU, GPU, MPU, ASIC, and processor
- Flowable silicone compound
-
DOWSIL 6-1104 CV SILICONE SEALANT
- Low-Outgassing Vacuum Sealing
- 610% Cured Elongation
- One-Part Moisture-Cure Sealing
-
DOWSIL™ 3-1953 Conformal Coating
- One-part, solventless silicone conformal coating
- UV indicator for inspection and quality assurance
- Soft, stress-relieving elastomer after cure
-
DOWSIL™ TC-5515 LT Low Density Thermal Conductive Gap Filler
- Low Density, Soft, & Compliant cured material
- Room-temperature cure in 360 minutes at 25°C
- Tacky surface after cure
-
DOWSIL™ TC-6010 Thermally Conductive Encapsulant
- Flowable and self-leveling formulation
- Excellent dielectric strength of 22 kV/mm
- 1.2 W/m·K thermal conductivity
-
DOWSIL 730 FS SOLVENT RESISTANT SEALANT
- One-Component Sealing System
- Room-Temperature Sealing Cure
- Non-Sag Placement Control
-
SYLGARD™ 160 Silicone Elastomer Kit
- Two-part silicone elastomer (1:1 mix ratio)
- Low shrinkage with no solvent byproducts
- Wide operating temperature range (-45°C to 200°C)
-
DOWSIL™ 3-1965 Conformal Coating
- One-part silicone conformal coating
- Flexible cure options: room temperature or heat-accelerated
- Wide operating temperature range (-55°C to 200°C)
-
DOWSIL™ TC-6040 Thermal Conductive Encapsulant
- Heat accelerated cure
- Room temperature cure
- 4.0 W/m·K flowable silicone encapsulant
-
-
SYLGARD™ 527 A&B Silicone Dielectric Gel
- 465 cP mixed viscosity for good flow under components
- Very soft, low-stress dielectric protection
- 425 V/mil dielectric strength and 2.75E+15 ohm*cm volume resistivity for electrical insulation
-
DOWSIL™ CC-8030 UV and Dual Moisture Cure Conformal Coating
- Low viscosity
- Dual cure system
- Soft elastomer after cure
-
DOWSIL™ TC-5533 Gap Filler
- Designed specifically for EV battery module
- Controlled siloxane volatility
- Vertical Stability
-
DOWSIL 732 MULTI-PURPOSE SEALANT
- One-Part Moisture-Cure Sealing
- Thermal Stability for Sealing
- Non-Sag Placement Control
-
DOWSIL EE-1010 LOW VISCOSITY ENCAPSULANT
- Low-Viscosity Encapsulant Application
- Controlled Cure Flexibility
- Firm Elastomeric Electrical Protection
-
SYLGARD™ 184 Silicone Elastomer Kit
- Two-part silicone elastomer (10:1 mix ratio)
- Flexible cure options: room temperature or heat-accelerated
- Low shrinkage and minimal internal stress
-
-
DOWSIL™ TC-5550 Thermal Conductive Compound
- Good pump-out resistance for bare die application
- High thixotropy
- Low thermal resistance
-
DOWSIL 733
- Non-Slumping Vertical/Overhead Application
- Primerless Glass, Metal, and Plastic Adhesion
- -57 to 177 deg C Flexibility
-
DOWSIL™ CC-8036 UV and Dual Moisture Cure Conformal Coating
- Dual Curing Mechanism
- High Viscosity Ideal for Needle Dispensing
- Silicone Conformal Coating
-
DOWSIL™ TC-4525 CV Thermally Conductive Gap Filler
- Controlled silicone volatility (CV)
- 2.5 W/m-K Thermal Conductivity
- Applicable for Vertical Position
-
-
-
DOWSIL™ 1-4105 Conformal Coating
- One-part, solventless silicone conformal coating
- Cures to a soft, low-stress elastomer
- Wide operating temperature range (-45°C to 200°C)
-
SYLGARD™ 170 Silicone Elastomer Kit
- Low mixed viscosity for flow into complex PCB assembly geometries
- Shore A 47 flexible elastomer for stress relief and mechanical protection
- UL 94 V-0 flame rating with 0.48 W/m·K thermal conductivity
-
-
-
DOWSIL 736
- Up to 260 deg C Continuous Service
- Non-Slumping Vertical/Overhead Application
- Flexible High-Temperature Silicone Sealing
-
-
DOWSIL™ TC-5860 Thermally Conductive Compound
- High dielectric strength
- 6.0 W/m-K Thermal Conductivity
- Suitable for High Power Electronics
-
DOWSIL 3-4155
- 60-Minute Gel Window
- Soft 60 G Gel for Dielectric Encapsulation
- 65 to 200 deg C Service Range
-
-
-
-
-
DOWSIL 738 ELECTRICAL SEALANT
- One-Part Moisture-Cure Sealing
- Non-Sag Placement Control
- 500% Cured Elongation
-
DOWSIL 3-4680
- Fast Room-Temperature Encapsulation Cure
- Low-Viscosity Dispensing Control
- Electrically Insulating Encapsulation
-
DOWSIL TC-4529
- One-Part Non-Curing Gap Filler
- Vertical-Position Retention
- Dispensable Thermal Gap Filling
-
DOWSIL™ EA-3838 Fast Adhesive (Base & Catalyst)
- Non-sag rheology
- Extreme temperature stability
- Flexible mix ratio
-
DOWSIL 3-6635 CLEAR DIELECTRIC GEL
- 80 to 200 deg C Service Range
- Ultra-Soft Dielectric Gel
- 20 kV/mm Dielectric Strength
-
DOWSIL Q1-4010 CONFORMAL COATING
- One-Part, Solventless Silicone Coating
- Multiple Supported Application Methods
- UV-Aided Coating Inspection
-
DOWSIL TC-8225 Thermally Conductive Gap Filler
- 2.7 W/(m K) Thermal Interface
- Soft, Compressible Silicone Gap Filler
- Automated Dispensing Ready
-
DOWSIL 748
- Non-Corrosive Application Formulation
- 15-Minute Tack-Free Time
- 55 to 177 deg C Service Range
-
DOWSIL ME-4039
- Transparent Addition-Cure Silicone Encapsulant
- 91.5% Transmission at 450 Nm
- 26-Minute 125 deg C Cure
-
DOWSIL TC-5021
- One-Part Non-Curing Thermal Compound
- 0.2 deg C cm^2/W Thermal Resistance
- 82,650 cP Application Viscosity
-
-
DOWSIL 340 SILICONE HEAT SINK GREASE
- Reworkable Thermal Interface Material
- Device-to-Heat-Sink Heat Transfer
- No-Mix No-Oven Processing
-
DOWSIL 744 RTV SILICONE SEALANT
- One-Part Moisture-Cure Sealing
- 70 psi Cured Tensile Strength
- Primerless Aluminum Bonding
-
DOWSIL™ 3-1944 HP RTV Coating
- One-Part, Solventless Silicone Coating
- 7-Minute Tack-Free Time
- Integrated UV Indicator
-
DOWSIL SE 4445
- Two-Component Electronics Silicone System
- White/Charcoal Component Identification
- 2.4 Relative Density
-
DOWSIL TC-4515
- 1.8 W/(m K) Thermal Conductivity
- 60-Minute Working Window
- 50 Shore 00 Hardness with Vertical-Hold Rheology
-
DOWSIL TC-5121C
- 2.8 W/(m K) Thermal Interface
- 0.09 deg C cm^2/W Thermal Resistance
- One-Part, Non-Curing and Flowable Formulation
-
-
DOWSIL TC-5622 THERMALLY CONDUCTIVE COMPOUND
- 4.3 W/(m K) Thermal Conductivity
- 0.06 deg C cm^2/W Thermal Resistance
- Non-Curing, Solventless Compound for Dispensing or Printing
-
-
DOWSIL TC-4535
- 3.4 W/(m K) Thermal Interface
- 60-Minute Working Window
- 52 Shore 00 Hardness with Vertical-Hold Rheology
-
DOWSIL TC-5351
- 3.3 W/(m K) Thermal Interface
- Screen-Printable Thermal Interface
- Vertical Gap-Fill Capability Up to 1.0 mm
-
-
DOWSIL SE 1816 CV
- Working Time Greater Than 1,440 Minutes
- 60-Minute Cure at 100 deg C
- Self-Priming Electronics Encapsulation
-
-
DOWSIL EA-9187L UV Conformal Coating
- One-Part Solvent-Free Silicone Coating
- Shore A 17 Hardness
- 20 kV/mm Dielectric Strength
-
DOWSIL 832
- Primerless Multi-Substrate Adhesion
- One-Part Low-Odor Neutral Cure
- -55 to 149 deg C Service
-
DOWSIL TC-5625C
- One-Part Non-Curing Thermal Interface Compound
- Thermally Conductive Thermal Interface
- Screen, Stencil, or Dispense Application
-
-
DOWSIL TC-4551
- 5.2 W/(m K) Thermal Conductivity
- 15-Minute Cure at 80 deg C
- Vertical-Position Retention
-
DOWSIL 1-4173 THERMALLY CONDUCTIVE ADHESIVE
- One-Part Heat-Cure Thermal Bonding
- 1.8 W/(m K) Thermal Bonding
- Primerless Thermal Bonding Processing
-
DOWSIL 786
- Mildew-Resistant High-Humidity Sanitary Sealant
- Permanently Flexible Cured Seal
- One-Part Non-Sag Application
-
DOWSIL TC-5888
- Thixotropic Application Control
- Thermally Conductive Thermal Interface
- Microprocessor and Power-Module Thermal Interfaces
-
-
DOWSIL CC-2588
- Five-Minute Tack-Free Processing
- 22.3 kV/mm Dielectric Strength
- Firm Abrasion-Resistant Cure
-
SYLGARD™ 164 Silicone Elastomer Kit
- Flowability for Different Processes
- Fast Room-Temperature Encapsulation Cure
- UL 94 V-0 Classification
-
DOWSIL SE 9186 Sealant
- Fast Room-Temperature Sealing Cure
- Self-Leveling Flowable Placement
- Controlled-Volatility Silicone Formulation
-
DOWSIL SC 102
- Moderate Thermal-Conductivity Compound
- One-Part Non-Curing Processing
- Critical-Component Heat Transfer
-
DOWSIL TC-6020
- Flowable Power-Electronics Encapsulation
- Moderate-Temperature Fast Cure
- 2.7 W/(m K) Thermal Protection
-
-
DOWSIL HC 1000 Gray Conformal Coating
- One-Part, Solventless Silicone Coating
- Room-Temperature Adhesive Cure
- 21 kV/mm Dielectric Strength
-
DOWSIL Q4-2805 NON-CURING FLUOROSILICONE CHANNEL SEALANT
- Aviation-Fuel, Fuel, and Oil Resistance
- Non-Curing, Catalyst-Free Formulation
- 55 to 200 deg C Service Range
-
DOWSIL 94-003
- One-Part Moisture-Cure Adhesive
- Fuel, Oil, and Moisture Resistance
- Brush, Dip, or Spray Application
-
DOWSIL TC-6032
- Extended-Flow Electronic Encapsulation
- 3.2 W/(m K) Thermal Protection
- EV Power-Component Encapsulation
-
DOWSIL Q4-2817 FLUOROSILICONE SEALANT
- 55 to 260 deg C Service Range
- Aviation-Fuel, Fuel, and Solvent Resistance
- Aerospace Sealing Application
-
-
DOWSIL SE 4420
- Fast 8-Minute Tack-Free Cure
- Manual or Automated Dispensing
- One-Part Thermal Module Bonding
-
DOWSIL TC-5080
- Non-Curing Thermal Grease
- Less Than 0.01% Oil Bleed After 24 Hours at 150 deg C
- Screen, Stencil, or Needle Application
-
DOWSIL SE 4450
- 1.9 W/(m K) Thermal Bonding
- Self-Leveling Flowable Placement
- 6.7 MPa Aluminum Lap Shear
-
DOWSIL 7092
- Immediate Green Strength
- One-Component, Neutral Moisture-Cure Formulation
- Flexible Cured Adhesive
-
DOWSIL SE 4485
- 2.8 W/(m K) Thermal Conductivity
- One-Part Moisture-Cure Silicone
- Thermal-Bonding Electrical Insulation
-
-
-
-
-
DOWSIL 90-006 RF
- Two-Hour Working Time at 25 deg C
- Mixing, Loading, Dispensing, and Assembly Processing
- Prepared/Primed Aerospace-Material Adhesion
-
-
DOWSIL HM-2600
- 115 to 135 deg C Application Range
- 15-Minute Open Time
- Greater Than 1200% Cured Elongation
-
DOWSIL TC-4015
- 1.7 W/(m K) Thermal Conductivity
- 4-Hour Working Time at 25 deg C
- Screen-Printed or Dispensed Gap Filling
-
DOWSIL 866 PRIMERLESS SILICONE ADHESIVE
- Primerless Silicone Adhesion
- Durable Silicone Formulation
- EV/Automotive Component Assembly
-
DOWSIL 9-1363
- Fast Skin-Over and Tack-Free Development
- Primerless Multi-Substrate Adhesion
- Neutral-Cure Silicone Adhesive
-
DOWSIL TC-4026
- Printable Formed-In-Place Thermal Pads
- Glass-Bead Thickness Control
- Soft Reworkable Thermal Interface
-
-
DOWSIL 9-1374
- One-Part Low-Odor Neutral Cure
- Primerless Multi-Substrate Adhesion
- -55 to 180 deg C Flexibility
-
-
DOWSIL TC-4040
- 4.0 W/(m K) Thermal Conductivity
- Cure in Less Than 5 Minutes at 120 deg C
- 60 um Minimum Bond Line
-
-
DOWSIL TC-4025
- Self-Leveling Dispensable Pad
- Approximately 2.5 W/(m K) Thermal Conductivity
- 30-Minute Cure at 125 deg C
-
SILASTIC 3-8186
- Low-Force Elastomeric Foam for Dispensed-in-Place Compression Gasketing
- Reduced-Flow Robotic Bead Dispensing
- 10-Minute 75 deg C Cure
-
DOWSIL 983
- Two-Part Structural Glazing Silicone
- +/-25% ASTM C719 Movement
- 10 to 25-Minute Working Window
-
-
DOWSIL PV-804
- One-Part Neutral Alkoxy Silicone Sealant
- 190 g/min Non-Slump Extrusion Rate
- 620% Cured Elongation
-
DOWSIL Q3-6611
- Self-Leveling Flowable Dispensing
- Temperature-Controlled Rapid Cure
- High Tensile Strength
-
-
DOWSIL SE 9160
- One-Part UV Cure With Secondary Moisture Cure
- Good Through (In-Depth) Curing in High UV Energy Density
- Faster In-Line Processing Through UV Curing
-
DOWSIL SE 9185
- Fast Tack-Free Room-Temperature Cure
- High Elongation for Stress Relief
- Controlled Silicone Volatility
-
DOWSIL SE 9187 L
- One-Part Moisture-Cure Adhesive
- Eight-Minute Tack-Free Time
- 20 kV/mm Dielectric Strength
-
DOWSIL SILASTIC Q3-3636 Adhesive
- Two-Component Fast-Cure Silicone
- Flexible Mix-Ratio Processing
- Low-Fogging Silicone Adhesive
-
-
-
DOWSIL 791
- +/-50% Weatherseal Movement
- Zero-Flow Weatherseal Application
- 20-Minute Weatherseal Tooling
-
DOWSIL 795
- Structural and Weatherseal Versatility
- Class 50 Glazing Movement
- 20-30-Minute Glazing Work Window
-
-
-
-
DOWSIL 3-8209
- 1:1 Silicone Foam Mixing
- 45 Shore 00 Cured Hardness
- Integrated Compression Gasket Formation
-
DOWSIL 3-8235
- Robotic Foam-Gasket Dispensing
- Heat Acceleration Below 100 deg C
- Low-Compression-Set Foam Sealing
-
DOWSIL 8257
- 1:1 Silicone Foam Mixing
- 25 Shore 00 Cured Hardness
- Integrated Compression Gasket Formation
-
SILASTIC 5-8733
- Fuel-Resistant Fluorosilicone Chemistry
- One-Part Cartridge Application
- 190% Cured Elongation
-
DOWSIL 739 PLASTIC ADHESIVE
- One-Part Adhesive System
- Flame-Resistant Cured Adhesive
- Non-Flowing Application Control
-
DOWSIL 236
- Durable, Dry-Surfaced Silicone Rubber Coating
- Sticky-Material Adhesion Prevention
- Multiple Application Methods
-
DOWSIL ME 1140 Silicone Adhesive
- Solvent-Free Bonding Formulation
- 60-Minute 130 deg C Cure
- Low-Modulus Cured Bonding
-
DOWSIL 92-009
- Room-Temperature Coating Cure
- Brush, Dip, Pour, and Spray Application
- Coating Build of 5 to 6 Mils
-
-
DOWSIL TC-2030 THERMALLY CONDUCTIVE ADHESIVE
- 2.7 W/(m K) Thermal Bonding
- Two-Part Heat-Cure Adhesive
- Electrical-Insulation Thermal Bonding
-
DOWSIL RSN-0804
- Hard Silicone Binder Resin
- 30 cP Resin Viscosity
- Short-Duration Heat-Resistant Coating Formulations
-
DOWSIL 3-0105
- Self-Priming Powertrain Sealing
- Noncorrosive Alkoxy RTV Cure
- One-Part Room-Temperature Gasket Cure
-
DOWSIL RSN-0805
- Decorative and Protective Coating Resin
- Enhanced Coating Softness and Flexibility
- Standalone or Blendable Resin Use
-
DOWSIL RSN-0806
- Colored Baking-Enamel Resin
- Up to 538 deg C Temperature Use
- Standalone or Blendable Resin Use
-
DOWSIL Q3-7062
- Excellent Unprimed Adhesion
- Remains Flexible over a Wide Temperature Range
- Excellent Weathering and Good Mechanical Properties
-
DOWSIL 280A
- Tack/Adhesion up to 260 deg C
- Solvent-Based Peroxide-Cure Silicone PSA
- Masking, Plating, and Splicing Tapes
-
DOWSIL 6-1125
- 0.025% Volatile Condensable Material
- 680% Cured Elongation
- 2.7 MPa Primed Aluminum Lap Shear
-
-
DOWSIL RSN-0996
- Motor/Coil/Transformer Impregnating Varnish
- 150 deg C Minimum Cure Temperature
- 1,626 V/mil Dielectric Strength
-
-
-
DOWSIL RSN-0997
- Silicone Impregnating Resin for Windings
- 90 to 120 cP Viscosity Range
- 2,000 V/mil Dry Dielectric Strength
-
-
DOWSIL 3-6876
- Flowable One-Part Processing
- 300-Minute 100 deg C Cure
- Balanced Cured Mechanical Properties
-
-
DOWSIL 1200
- No-Mix Primer Application
- RTV and Heat-Cure Silicone Adhesion
- Glass, Ceramic, FR-4, and Metal Adhesion
-
DOWSIL DA6534
- 6.8 W/(m K) Thermal Conductivity
- Electrically Conductive Bonding
- One-Part Heat-Cure Bonding
-
DOWSIL 1201
- Adhesion-Promoting Surface Treatment
- Low-Viscosity Adhesive Application
- 1 to 2-Hour Cure Window
-
DOWSIL 3-6060
- Improved Inhibition Resistance
- Promotes Bonding to Most Plastics
- Wipe, Dip, or Spray Application
-
-
-
DOWSIL 92-023
- Adhesion-Promoting Surface Treatment
- Improved Inhibition Resistance in Addition-Cure Silicone Systems
- 1 to 2-Hour Cure Window
-
DOWSIL Q2-3067
- One-Part Grease-Like Optical Couplant
- Fiber-Optic Assembly Applications
- Above 101.1 deg C Flash Point
-
DOWSIL DS-1000
- Silicone Oil/Grease/Elastomer Emulsification
- Immersion, Recirculation, or Spray Cleaning
- Above 100 deg C Flash Point
-
-
-
-
DOWSIL OS-30
- Complete Low-Residue Room-Temperature Evaporation
- Low-Surface-Tension Precision Cleaning
- Most-Plastic and Coating Compatibility
-
DOWSIL SE 9120
- Ready-to-Dispense Flowable Silicone Sealant
- Fast Tack-Free No-Mix Processing
- Controlled-Volatility Electronics/Industrial Sealant
-
DOWSIL P5200
- RTV and Heat-Cure Adhesion Promotion
- Wipe, Dip, or Spray Application
- 18-Month Shelf-Life Indicator
-
-
DOWSIL PR-2260 PRIME COAT CLEAR RTV SILICONE
- Adhesion-Promoting Surface Treatment
- Thin-Film Silane Primer
- Electronics and Industrial Assembly Applications
-
-
DOWSIL 1-2620LV
- Low-Viscosity Narrow-Gap Coating
- Room-Temperature Moisture Cure
- UV-Aided Automated Inspection
-
DOWSIL PR1200
- Adhesion-Promoting Surface Treatment
- Wipe, Spray, or Dip Application
- 1 to 2-Hour Cure Window
-
DOWSIL SE 9189 L
- One-Part Flowable RTV Silicone Adhesive
- Eight-Minute Tack-Free Time
- 25 kV/mm Dielectric Strength
-
DOWSIL PR1204
- Adhesion-Promoting Surface Treatment
- Light, Even Application by Wiping, Dipping
- Room-Temperature Adhesive Cure
-
DOWSIL X3-1598
- UV-Indicator Flowable Silicone Adhesive
- 60-Minute 125 deg C Cure
- Primerless Aluminum Bonding
-
DOWSIL PR4040
- Adhesion-Promoting Surface Treatment
- One-Part Surface Preparation System
- Clear Primer Dispersed in Heptane
-
DOWSIL 282
- High-Adhesion Tape Formulation
- 55-57% Active Silicone Content
- Cured-Film Electrical Insulation
-
DOWSIL 3-4088
- 4.5-Minute Working Time
- Low-Viscosity Under-Component Flow
- Soft Dielectric Gel Protection
-
-
-
-
DOWSIL ME-4131
- One-Part Clear Addition-Cure Silicone Coating for Die Coating
- 6,575 cP Application Viscosity
- 19 kV/mm Dielectric Strength
-
DOWSIL 995
- 350 psi Ultimate Tensile Strength
- +/-50% Structural Joint Movement
- 10-20-Minute Structural Glazing Window
-
DOWSIL ME-4132
- One-Part Black Microelectronics-Grade Silicone Encapsulant for Sensors
- 138% Cured Elongation
- Low-Modulus Cured Encapsulation
-
DOWSIL Q3-6575
- Clear 1:1 Dielectric Gel System
- 750 cP Mixed Viscosity
- Room-Temperature Encapsulation Cure
-
DOWSIL DA-6534
- 6.8 W/(m K) Thermal Conductivity
- 1.8E-04 ohm-cm Volume Resistivity
- One-Part Silver-Filled Silicone
-
-
DOWSIL EA 7100
- 15-Minute Cure at 100 deg C
- More Than 24-Hour Pre-Cure Window
- Aluminum and PBT Adhesion Data
-
-
DOWSIL PV-801
- Non-Slump PV Frame Sealing
- 746% Elongation for Flexible Sealing
- Glass and Backsheet Junction-Box Bonding
-
-
DOWSIL Q2-7406
- Silicone PSA Tape Coating
- High-Temperature Tape Adhesion
- Adjustable Tack-Cohesion Balance
-
-
DOWSIL Q3-3384-1
- Visual 10:1 Mix Verification
- Fast Room-Temperature Handling
- Non-Self-Leveling Component Sealing
-
DOWSIL Q3-6679
- Fuel- and Solvent-Resistant Insulation
- Extended Working-Time Processing
- Flexible Room-Temperature or Heat Cure
-
-
-
DOWSIL SE4400
- Extended 17-Hour Working Window
- Accelerated 30-Minute Heat Cure
- Thermally Conductive PCB Bonding
-
DOWSIL 3-1818
- Glass-Bead Bondline Control
- 1.68 W/(m K) Thermal Conductivity
- 10-Minute Cure at 150 deg C
-
-
-
-
DOWSIL EE-9100
- 23-Minute Pot Life at 25 deg C
- 25 kV/mm Dielectric Strength
- 0.31 W/(m K) Thermal Conductivity
-
DOWSIL SE 4422
- 11-Minute Tack-Free Time
- 0.9 W/(m K) Thermal Conductivity
- Semi-Flowable One-Part Application
-
-
-
DOWSIL LPA-4000
- One-Part Non-Slumping RTV Silicone
- Spray, Trowel, Brush, or Roller Application
- Thermally Conductive Coating
-
-
DOWSIL EE-9000
- 130-Minute Pot Life at 25 deg C
- 23 kV/mm Dielectric Strength
- 0.2 W/(m K) Thermal Conductivity
-
DOWSIL ME-6820
- Low-Ionic Wire-Bond Encapsulation
- 60-Minute Cure at 150 deg C
- 18 kV/mm Dielectric Strength
-
DOWSIL SE 4410
- 6-Hour Pot Life at 25 deg C
- 0.92 W/(m K) Thermal Conductivity
- 24 kV/mm Dielectric Strength
-
-
-
-
SILASTIC RTV-3120
- 28,000 cP Base Viscosity
- High-Temperature Mold Service