DOWSIL RSN-0233
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 99% Solids Flake Resin
- 500 cP at 140 deg C
- 21-Month Usable Life
Product Description
DOWSIL RSN-0233 Flake Resin is a 100% silicone, silanol-functional solid resin used as a binder or co-binder in powder and liquid coating formulations. Typical properties include 99% solids, 1.32 specific gravity at 25 deg C, and 500 cP melt viscosity at 140 deg C. The resin is used to improve heat stability and weatherability in powder coatings and to provide initial and hot hardness in high-temperature coatings. It can also be blended with silicone or solvent-based organic resins to improve hardness or film properties. The product has a 21-month usable life when stored at or below 30 deg C in the original unopened container.
Key features
- Silanol-Functional Silicone Binder: The 100% silicone flake resin is used as a powder-coating binder or co-binder.
- About 99% Solids Content: Typical specific gravity is about 1.32.
- About 500 cP Melt Viscosity at 140 deg C: The value characterizes the resin in its molten processing state.
Applications
Binder or co-binder for heat-stable and weatherable coatings; high-temperature coatings; silicone- and organic-resin blending.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Solids content | 99 | % | Typical |
| Specific gravity | 1.32 | 25 deg C | |
| Melt viscosity | 500 | cP | 140 deg C |
| Flash point | 138 | deg C | Closed cup |
| Hydroxyl content | 6.0 | % | Typical |