DOWSIL Q3-7062
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Excellent Unprimed Adhesion
- Remains Flexible over a Wide Temperature Range
- Excellent Weathering and Good Mechanical Properties
Product Description
DOWSIL™ Q3-7062 RTV Silicone Rubber is a one-part, neutral-cure RTV silicone rubber designed for sealing and bonding industrial assemblies that contain dissimilar materials with different thermal expansion rates. This non-corrosive, non-slumping silicone adhesive provides excellent unprimed adhesion to most metals and many plastics while maintaining flexibility across a wide temperature range. The material offers strong weatherability, good mechanical properties, and outstanding UV resistance, making it suitable for automotive lamp assembly and a variety of industrial sealing and bonding applications where durable, flexible bonds are required.
Key features
- Neutral-cure silicone chemistry: One-part, non-corrosive formulation that simplifies dispensing and application processes.
- Excellent adhesion: Bonds to most metals and many plastics without primer in many applications.
- UV and weather resistance: Maintains performance in outdoor and exposed environments requiring long-term durability.
Applications / Suitable for
- Automotive lamp sealing and bonding
- Industrial assembly sealing
- Bonding dissimilar materials
- Applications requiring flexible, durable seals
- Outdoor assemblies exposed to weathering and UV radiation
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied properties measured at 23°C and 50% relative humidity.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Consistency | Non-slumping paste | — | CTM 0176 |
| Color | Black | — | Black grade |
| Skin-over Time | 30 | min | CTM 0098 |
| Tack-free Time | 50 | min | CTM 0095 |
| Cure Rate | 2 | mm/24 h | 23°C, 50% RH |
| Specific Gravity | 1.5 | — | CTM 0097 |
After-processing / final-state properties
Typical cured properties after 7 days at 23°C and 50% relative humidity.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Durometer Hardness | 37 | Shore A | ASTM D2240 |
| Tensile Strength | 1.5 | MPa | ASTM D412 |
| Elongation | 650 | % | ASTM D412 |
| Lap Shear Adhesion (PC to PC) | 1.05 | MPa | ASTM D816 |