Vibra-TITE MP-55330

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

Vibra-TITE MP-55330

Main features

  • Extended 25- to 30-Minute Work Time
  • Equal-Ratio Resin Mixing
  • Structural Plastic and Metal Bonding

Product Description

MP55330 Methacrylate Adhesive is a two-component adhesive with resin and activator mixed 1:1 by volume or weight for bonding plastics, metals, and composite assemblies. It provides a 25 to 30 minute work time for part alignment, followed by handling strength in 40 to 60 minutes. Resin and activator viscosities are 70,000 and 50,000 cps at 25 deg C. Cured shear and tensile strength are each 3,000 to 3,500 psi; test methods are unspecified. For consistent dispensing, the recommended material-temperature window is 65 to 80 deg F, and the adhesive cures at room temperature.

Key features

  • Extended Alignment Window: Work time is 25 to 30 minutes before handling strength develops in 40 to 60 minutes.
  • Equal-Ratio Mixing: Resin and activator mix 1:1 by volume or weight.
  • Structural Strength Range: Cured shear and tensile strength are 3,000 to 3,500 psi; test methods are unspecified.

Applications

Bonding plastics, metals, and composite assemblies.

Product Family

VIBRA-TITE MP-55330

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methyl Methacrylate (MMA)
Density (g)
0.98 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Physical Properties
Viscosity (Part A)
60,000 - 80,000 mPa.s
Viscosity (Part B)
60,000 - 110,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Component and process-window values apply to the exact 1:1 MP55330 resin and activator system.

PropertyValueUnitMethod / condition
Viscosity - resin70,000cps25 deg C; value status not stated
Viscosity - activator50,000cps25 deg C; value status not stated
Volume mix ratio1 to 1RatioResin to activator
Weight mix ratio1 to 1RatioResin to activator
Thixotropic index5UnitlessMethod not stated
Work time25 to 30minCondition not stated
Handling strength40 to 60minCondition and threshold not stated
Gap fill0.125inListed dimension
Technical properties

Final-state properties

PropertyValueUnitMethod / condition
Shear strength3,000 to 3,500psiCured value; method and substrate not stated
Tensile strength3,000 to 3,500psiCured value; method not stated
Temperature range-67 to 250deg FService basis not stated