TECHNOMELT 1X

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

HYSOL 1X

Main features

  • Fast 15-Second Open Time
  • Porous-Substrate Hot-Melt Bonding
  • High Dielectric Strength

Product Description

TECHNOMELT 1X is an EVA-based, medium-to-fast-setting hot-melt adhesive recommended for porous substrates. Its one-part format bonds paper, wood, fabric, nonwovens, and foam, with a typical open time of 15 seconds. At 350 deg F, typical viscosity is 2,000 cP, while the softening point is 216 deg F. Typical material properties include 370 psi tensile strength, 90% elongation, and dielectric strength above 1,300 V/mil. This short-open-time profile is tailored to paper, wood, fabric, nonwoven, and foam bonding.

Key features

  • Fast open time: Typical open time is 15 seconds.
  • Porous-substrate bonding: Recommended substrates include paper, wood, fabric, nonwovens, and foam.
  • Dielectric strength: Typical dielectric strength is above 1,300 V/mil by ASTM D149.

Applications

Bonding paper, wood, fabric, nonwovens, and foam.

Technical Specifications

Physical Properties
Open time
0.25 minutes
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2,000 mPa.s
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.96
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
90 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical product-selection data and are not specifications.

PropertyValueUnitMethod / condition
Softening point216deg FASTM E28-67; typical
Viscosity2,000cP350 deg F; ASTM D3236; typical
Open time15secTypical
Specific gravity0.9677 deg F; ASTM D792; typical
Technical properties

After-processing / final-state properties

Values describe the cured material and are typical product-selection data, not specifications.

PropertyValueUnitMethod / condition
Heat resistance150deg FASTM D4498; typical
Tensile strength370psiASTM D638; typical
Elongation90%ASTM D638; typical
Glass transition temperature-21deg FASTM E1640; typical
Dielectric strengthAbove 1,300V/milASTM D149; typical