PERMABOND HH040
Harmonization Code : 8001.20 | Unwrought tin: Tin alloys
Main features
- 5,000 mPa s Retaining Viscosity
- General-Purpose Maximum Gap Fill
- 14 MPa Retaining Shear
Product Description
PERMABOND HH040 is a single-component anaerobic retaining compound for close-fitting cylindrical metal assemblies. Viscosity is 5,000 mPa s and shear strength is 14 MPa, with general-purpose retaining and maximum-gap filling within its product class. The adhesive is used to retain and seal cylindrical metal parts, including shaft-and-hub type assemblies, where anaerobic cure is appropriate. Its 5,000 mPa s viscosity gives the adhesive a higher-body profile for controlled placement in cylindrical interfaces. HH040 combines retaining strength, sealing function and gap-filling capability for close-fitting cylindrical metal joints.
Key features
- 5,000 mPa s Retaining Grade: Viscosity provides a higher-body anaerobic profile for cylindrical metal assemblies.
- 14 MPa Shear Strength: Shear strength is 14 MPa for the retaining compound.
- Maximum-Gap Filling: The retaining compound is intended for general-purpose use with maximum-gap filling within its product class.
Applications
Retaining and sealing close-fitting cylindrical metal parts, including shaft-and-hub type assemblies.