MOLYKOTE L-4611
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Dedicated Reciprocating-Compressor Lubrication
- Temperature-Indexed Diester Viscosity
- Rust and Oxidation Protection
Product Description
MOLYKOTE L-4611 Synthetic Reciprocating Compressor Oil is an ISO VG 100 diester synthetic lubricant for reciprocating compressor service. Typical kinematic viscosity is 98 cSt at 40 deg C and 9.5 cSt at 100 deg C, with a viscosity index of 62 and a pour point of -28 deg C. The grade uses a rust-and-oxidation additive package and has a typical specific gravity of 0.960 at 20 deg C. The L-4611 grade is for reciprocating compressors that specify this exact diester oil.
Key features
- Reciprocating-Compressor Focus: The ISO VG 100 oil is specified for reciprocating compressor lubrication.
- Diester Base-Oil System: The synthetic grade uses diester base oil with rust-and-oxidation additives.
- Temperature-Indexed Viscosity: Typical viscosity is 98 cSt at 40 deg C and 9.5 cSt at 100 deg C.
Applications
Reciprocating compressors.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical values; not for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| ISO viscosity grade | 100 | - | Manufacturer designation |
| Kinematic viscosity | 98 | cSt | Typical at 40 deg C |
| Kinematic viscosity | 9.5 | cSt | Typical at 100 deg C |
| Viscosity index | 62 | - | Typical |
| Pour point | -28 | deg C | Typical |
| Specific gravity | 0.960 | - | Typical at 20 deg C |
| Base oil | Diester | - | Typical composition |
| Additive package | R&O | - | Typical composition |