MOLYKOTE L-2115

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

MOLYKOTE L-2115

Main features

  • Extreme-Pressure Enclosed-Gear Lubrication
  • Micropitting-Focused PAO Protection
  • Rapid 10-Minute Water Separation

Product Description

MOLYKOTE L-2115 Synthetic Gear Oil is a fully synthetic ISO VG 150 PAO gear oil for industrial gear units requiring an extreme-pressure lubricant. Typical kinematic viscosity is 162 cSt at 40 deg C and 18.2 cSt at 100 deg C, with a viscosity index of 128. The formulation combines a sulfur-phosphorous EP additive with corrosion inhibition and is designed for spur, helical, bevel, and planetary gears, including severe conditions where micropitting is a concern. Water separation is assessed by ASTM D1401 demulsibility testing, and load performance by FZG load-stage testing, for demanding enclosed-gear service.

Key features

  • ISO VG 150 Gear Protection: The PAO grade combines sulfur-phosphorous EP additives with corrosion inhibition.
  • Micropitting-Focused Formulation: The synthetic gear oil is designed for severe conditions where micropitting is a concern.
  • Load and Water Separation: Typical results include greater than 12 FZG load stage and 40/40/0 demulsibility at 10 minutes.

Applications

Enclosed industrial spur, helical, bevel and planetary gear drives where the specified viscosity grade is required.

Product Family

MOLYKOTE L-2115

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density
Volumetric mass per unit
0.845 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
238 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values; not for use in preparing specifications.

PropertyValueUnitMethod / condition
ISO viscosity grade150-Manufacturer designation
Kinematic viscosity162cStASTM D445 at 40 deg C
Kinematic viscosity18.2cStASTM D445 at 100 deg C
Viscosity index128-ASTM D2270
Pour pointLess than -43deg CASTM D97
Water contentLess than 500ppmISO 3733
Demulsibility40/40/0mL/mL/mLASTM D1401; 10 min
FZG failure load stageGreater than 12-DIN 51354-2; A/8.3/90