MOLYKOTE G-1056

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-1056

Main features

  • Automotive Noise-Reduction Lubrication
  • No-Oil-Bleed PAO Formulation
  • Power Slide-Door Coverage

Product Description

MOLYKOTE G-1056 Grease is a yellow NLGI 1 PAO-based grease with a lithium-complex thickener and PTFE solid lubricant. It is designed for lubrication and noise reduction in automotive body and interior components, including power slide-door rails and actuators. The service-temperature range is -40 to 150 deg C. The grease combines compatibility with most plastics, shear stability, no oil bleed, reduced noise and vibration, and reduced separated-oil contamination. These characteristics apply to this grease under the specified automotive contact conditions.

Key features

  • Automotive noise-reduction lubrication: Supports lubrication and noise reduction in supported body and interior components.
  • No-oil-bleed formulation: Uses a low-bleed PAO formulation to reduce separated-oil contamination in supported assemblies.
  • Power slide-door coverage: Lubricates supported power slide-door rails and actuators in automotive applications.

Applications

Applications include automotive power slide-door rails and actuators, plus supported body and interior components requiring lubrication and noise reduction.

Product Family

MOLYKOTE G-1056

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Yellow

Additional Information

Technical properties

As-supplied / before-processing properties

Selection properties are limited to the exact manufacturer product page; no neighboring grease values are transferred.

PropertyValueUnitMethod / condition
ColorYellow-Manufacturer product details
Consistency1NLGI gradeManufacturer product details
Base-oil technologyPolyalphaolefin (PAO)-Manufacturer product details
ThickenerLithium complex-Manufacturer product details
Solid lubricantPTFE-Manufacturer product details