MOLYKOTE G-0051 FM

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-0051

Main features

  • NSF H1 Incidental-Contact Lubrication
  • High-Load NLGI 1 Grease
  • Food-Machinery Bearing Coverage

Product Description

MOLYKOTE G-0051 FM White EP Bearing Grease is a white NLGI 1 mineral-oil grease with an aluminum-complex thickener and extreme-pressure and anti-wear additives. It is formulated for bearings, chains, gears and slides in food and beverage machinery where incidental food contact may occur. The grease has NSF H1 registration and complies with FDA 21 CFR 178.3570. Typical grade-specific properties include 325 penetration, 99 cSt base-oil viscosity at 40 deg C, and a 7,845 N four-ball weld load. The service-temperature range is -17 to 150 deg C.

Key features

  • NSF H1 incidental-contact lubrication: Lubricates supported food-processing points where incidental food contact may occur.
  • High-load NLGI 1 grease: Combines an NLGI 1 consistency with extreme-pressure and anti-wear additives.
  • Food-machinery bearing coverage: Fits supported bearings, chains, gears and slides in food and beverage equipment.

Applications

Applications include supported bearings, chains, gears and slides in food and beverage machinery requiring NSF H1 incidental-contact lubricant selection.

Product Family

MOLYKOTE G-0051 FM

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1.05 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are exact to the G-0051 FM NLGI 1 grade; neighboring G-0050 FM and G-0052 FM values are not used.

PropertyValueUnitMethod / condition
ColorWhite-Typical; exact G-0051 FM grade
Consistency1NLGI gradeASTM D217 classification
Penetration3250.1 mmASTM D217; typical
Density1.05g/mlTypical at 20 deg C
Base-oil viscosity99cStTypical at 40 deg C
Dropping point256deg CTypical; not an operating-temperature limit
Four-ball weld load7845NTypical; exact G-0051 FM grade
Water washout4%Typical at 175 deg F