MOLYKOTE AI-6159

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE AI-6159

Main features

  • Automotive Plastic Noise Control
  • Window-Regulator Guide Lubrication
  • -40 to 150 deg C Range

Product Description

MOLYKOTE AI-6159 Grease is a white PAO-based lithium grease containing PTFE and additives for lubrication and noise control in automotive plastic sliding components. Applications include window-regulator guides and other supported sliding parts. The grease has a service-temperature range of -40 to 150 deg C and may be applied by brush, spatula or automated equipment. Typical properties include 305 worked penetration, 1.9% bleed after 24 hours at 100 deg C, and a 0.61 mm four-ball wear scar under the stated test conditions.

Key features

  • Automotive plastic noise control: Supports lubrication and noise reduction in supported automotive plastic sliding components.
  • Window-regulator guide lubrication: Fits window-regulator guides and other supported sliding parts in automotive assemblies.
  • -40 to 150 deg C range: Has this service-temperature range for the supported applications.

Applications

Applications include automotive window-regulator guides and other supported plastic sliding components requiring lubrication and noise reduction.

Technical Specifications

General Properties
Evaporation Rate
0.2% @ 99°C, 22 h
Thermal Properties
Service temperature
−40 to +150°C °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical grease and test values apply to MOLYKOTE AI-6159 Grease under the stated conditions.

PropertyValueUnitMethod / condition
ColorWhite-Typical; as supplied
Worked penetration3050.1 mmTypical; 60 strokes
Bleed1.9%Typical; 24 hours at 100 deg C
Evaporation0.2%Typical; 22 hours at 99 deg C
Four-ball wear scar0.61mmASTM D2266; 1,200 rpm, 392 N, 1 hour
Copper corrosion1aratingTypical; 24 hours at 100 deg C
Low-temperature starting torque290mN-mTypical at -40 deg C
Low-temperature running torque130mN-mTypical at -40 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers