LORD MAXLOK T3S

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

LORD MAXLOK T3S

Main features

  • 3 to 5 Minute Work Time
  • 6 to 8 Minute Handling
  • Non-Sag Structural Placement

Product Description

LORD Maxlok T3S Acrylic Adhesive is a fast-working two-component structural acrylic adhesive used with LORD Maxlok MX accelerator for bonding supported metals and composites. Its off-white to tan paste formulation is part of the Maxlok S-series offered as an alternative to welding, brazing, riveting and other mechanical fastening methods in assemblies exposed to high impact or peel loads. T3S provides 3 to 5 minutes of working time and reaches handling strength in 6 to 8 minutes at 77 deg F (25 deg C). The non-sag system supports cartridge or automatic dispensing and has a service-temperature range of -40 deg F to 300 deg F (-40 deg C to 149 deg C).

Key features

  • Fast T3S work time: Provides 3 to 5 minutes for rapid assembly at 77 deg F (25 deg C).
  • Rapid handling strength: Reaches 50 psi handling strength in 6 to 8 minutes at 77 deg F (25 deg C).
  • Non-sag structural placement: Supports cartridge or automatic application on vertical and overhead bond areas.

Applications

Applications include structural bonding of supported metals and composites as an alternative to selected mechanical fastening methods.

Technical Specifications

General Properties
Color
The color
Gray Paste
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:4 by Volume

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system values apply specifically to Maxlok T3S adhesive with MX accelerator.

PropertyValueUnitMethod / condition
Component appearanceOff-white to tan paste; grey paste-T3S adhesive; Maxlok MX accelerator
Adhesive viscosity70,000 to 200,000cPTypical; Brookfield at 77 deg F (25 deg C); T3S adhesive
Accelerator viscosity100,000 to 500,000cPTypical; Brookfield at 77 deg F (25 deg C); Maxlok MX accelerator
Adhesive density8.25 to 8.75lb/galTypical; T3S adhesive
Flash point59 (15)deg F (deg C)Typical; T3S adhesive
Working time3 to 5minutesTypical; T3S/MX system at 77 deg F (25 deg C)
Time to handling strength6 to 8minutesTypical; 50 psi shear; T3S/MX system at 77 deg F (25 deg C)
Shelf life9monthsEach component; original unopened container below 80 deg F (27 deg C)
Technical properties

After-processing / final-state properties

Final-state characteristics apply to the cured Maxlok MX/T3S system within the stated manufacturer scope.

PropertyValueUnitMethod / condition
Service temperature-40 to 300deg FDocumented performance range for Maxlok MX/T3S (-40 to 149 deg C)
Environmental resistanceResistant-Cured system; qualitative resistance to dilute acids, alkalis, solvents, greases, oils, moisture, salt spray and weathering
Indirect UV resistanceExcellent-Cured system; qualitative characteristic