LOCTITE UR 8540
Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other
Main features
- 110-Minute Open Time
- 5,500 mPa s Viscosity
- 100% Solids Content
Product Description
LOCTITE UR 8540 is a one-component, solvent-free liquid polyurethane laminating adhesive that moisture cures without a component-mixing step. Typical uncured properties include 1.08 g/cm^3 density, 100% solids, and 5,500 mPa s viscosity at 25 deg C. At 24 deg C, typical open time is 110 minutes and typical press time is 140 minutes. The adhesive can be applied by bead extrusion or manual troweling. Because cure depends on moisture, at least one substrate must be porous or perforated. Pressing is required during moisture cure to maintain contact between the laminated elements.
Key features
- Lamination Open Time: Typical open time is 110 minutes at 24 deg C.
- Application Rheology: Typical uncured viscosity is 5,500 mPa s at 25 deg C.
- Solvent-Free Solids: Typical uncured solids content is 100%.
Applications
Sandwich-panel lamination with wood, lauan, fiberboard, particle board, plywood, FRP, EPS foam, PU foam, and primed metals; structural lamination for RVs, motor homes, and trailers.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Density | 1.08 | g/cm^3 | Typical uncured material at 25 deg C |
| Solids | 100 | % | Typical uncured material |
| Viscosity | 5,500 | mPa s | Typical uncured material at 25 deg C |