LOCTITE SF 7515

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

LOCTITE SF7515

Main features

  • No-Rinse Spray or Wipe
  • 20 to 40 deg C Application
  • Aluminum, Zinc, and Steel Pretreatment

Product Description

LOCTITE SF 7515 is a one-part, amber, water-based surface treatment for temporary flash-rust protection and metal pretreatment before coating. Supported metal surfaces include aluminum, zinc, zinc alloy, cold-rolled steel, and blasted metal. Apply the no-rinse treatment by spray or wipe to a clean surface at 20 to 40 deg C. Remove excess as needed and allow the thin film to dry. Typical as-supplied density is 1.01 g/cm^3 and pH is 2.1 to 2.7.

Key features

  • No-Rinse Spray or Wipe: Apply to clean metal, remove excess as needed, and allow the film to dry without rinsing.
  • Temperature-Controlled Application: Apply at 20 to 40 deg C.
  • Aluminum, Zinc, and Steel Pretreatment: Supported surfaces include aluminum, zinc, zinc alloy, cold-rolled steel, and blasted metal.

Applications

Temporary flash-rust protection and metal pretreatment before coating on aluminum, zinc, zinc alloy, cold-rolled steel, and blasted metal surfaces.

Product Family

LOCTITE SF 7515

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber liquid
Chemistry Type
Hexafluorotitan acid
Density (g)
1.01 g/cm3

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
AppearanceAmber liquidTDS; as supplied
Density1.01g/cm^3Typical TDS value
pH2.1 to 2.7Typical TDS value