LOCTITE PE 3162
Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations
Main features
- Dedicated PE Hardener Component
- Amber Liquid Component Identification
- Estimated Zero VOC Content
Product Description
LOCTITE PE 3162 Epoxy Hardener is the liquid hardener component for compatible LOCTITE PE 3141 and PE 3142 epoxy potting systems. The amber, alkaline liquid has a relative density of 1.0 and an estimated VOC content of 0%, providing clear as-supplied identification during component preparation. It is supplied as the curing component only and must be combined with the applicable resin under the system's validated mixing and cure instructions. Applications include hardener service in supported PE epoxy potting assemblies using PE 3142 or compatible PE resin systems; resin properties and cured-system performance are excluded from this component page.
Key features
- Dedicated Hardener Component: Supplied as the PE 3162 curing component for compatible PE epoxy potting resin systems.
- Amber Liquid Identification: The amber liquid and relative density of 1.0 keep the component identity explicit during preparation.
- Estimated Zero VOC Content: As-supplied VOC content is estimated at 0% and 0 g/L.
Applications
Hardener component for LOCTITE PE 3142 and compatible PE epoxy potting resin systems.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Values apply only to the LOCTITE PE 3162 hardener component as supplied.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Physical state | Liquid | As supplied | |
| Color | Amber | As supplied | |
| pH | Alkaline | As supplied | |
| Relative density | 1.0 | Dimensionless | As supplied |
| Flash point | 118.33 | deg C | Closed cup |
| VOC content | 0 | % | Estimated; 0 g/L |