LOCTITE PC7319
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- 28 to 40 Minute Gel Time
- -30 to 120 deg C Dry Service
- Brush- or Roller-Applied Coating
Product Description
LOCTITE PC 7319 is a two-component epoxy coating for chemical-corrosion protection of industrial equipment and concrete surfaces. The gray mixed liquid can be applied by brush or roller after resin and hardener are combined at 2.3:1 by volume or 3.4:1 by weight. At 25 deg C, gel time is 28 to 40 minutes and recoat time is 1 to 4 hours. Typical dry service temperature is -30 to 120 deg C. Cured material has Shore D 85 hardness, 0.421 W/(m K) thermal conductivity, and 68 N/mm^2 compressive strength.
Key features
- Chemical-Exposure Coating: Used on equipment and concrete surfaces exposed to aggressive chemicals, including sulfuric-acid exposure service.
- Gel and Recoat Timing: Gel time is 28 to 40 minutes at 25 deg C, with a 1 to 4 hour recoat window at the same temperature.
- -30 to 120 deg C Dry Service: Typical dry service temperature spans -30 to 120 deg C.
Applications
Tanks, chutes, chemical-containment areas, concrete pits, tanks, floors, foundations, and related surfaces exposed to aggressive chemicals.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Resin viscosity | 40,000 to 60,000 | mPa s | Brookfield RV, spindle 7, 20 rpm, 25 deg C |
| Hardener viscosity | 400 to 850 | mPa s | Brookfield RV, spindle 3, 20 rpm, 25 deg C |
| Mixed viscosity | 5,000 | mPa s | Cone and plate, shear rate 10 s^-1, 25 deg C |
| Mixed density | 1.43 | g/cm^3 | 23 deg C |
| Mix ratio by volume | 2.3:1 | Resin:hardener | |
| Mix ratio by weight | 3.4:1 | Resin:hardener |
Cured material
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shore hardness | 85 | Shore D | ISO 868, cured material |
| Thermal conductivity | 0.421 | W/(m K) | ASTM F433, cured material |
| Glass transition temperature | 56 | deg C | ISO 11359-2, cured material |
| Compressive strength | 68 | N/mm^2 | ISO 604, cured material |
| Tensile strength | 33 | N/mm^2 | ISO 527-2, cured material |
| Elongation at break | 1.0 | % | Cured material |
| Lap shear strength | 18.2 | N/mm^2 | ISO 4587, grit-blasted mild steel |