LOCTITE MR 5922
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 500,000 to 700,000 mPa s Viscosity
- 24-Hour Full Cure
- Preformed Gasket Repair
Product Description
LOCTITE MR 5922 is a one-part, slow-drying solvent-based gasket sealant paste for flanges, fittings, connections, flexible assemblies, and dressing or repairing preformed gaskets. It cures by solvent evaporation. Typical as-supplied properties include specific gravity 1.5 at 25 deg C, Brookfield viscosity of 500,000 to 700,000 mPa s at 25 deg C, and approximately 87% solids by weight. The slower-drying formula increases work time. After application, the assembly is operational after 4 hours, and full cure occurs after 24 hours.
Key features
- 500,000 to 700,000 mPa s Viscosity: Brookfield RVT viscosity at 25 deg C, spindle 7, 5 rpm.
- Cure Completion: Full cure occurs after 24 hours.
- Preformed Gasket Repair: The sealant dresses or repairs damaged pre-cut gaskets.
Applications
Sealing flanges, fittings, connections, flexible assemblies, and dressing or repairing preformed gaskets.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 1.5 | Typical; 25 deg C | |
| Viscosity | 500,000 to 700,000 | mPa s | Typical; Brookfield RVT, 25 deg C, spindle 7, 5 rpm |
| Solids content | Approximately 87 | % by weight | Typical |