LOCTITE MR 5426

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE MR5426MAXIMUM

Main features

  • 5-Minute Minimum Dry Time
  • 30-Minute Bonding Window
  • Adjustable Spray-Pattern Control

Product Description

LOCTITE MR 5426 is an aerosol headliner spray adhesive for bonding foam, carpet, fabrics, plastics, and rubber in interior trim assemblies. The spray pattern can be set to low, medium, or high, with 2 to 3 overlapping coats applied from 6 to 8 inches. Allow a minimum of 5 minutes between coats and at least 5 minutes, or until tacky, before setting. Assemble the bond within 30 minutes of application. Typical uses include headliners, carpets, trunk linings, and door panels, and the adhesive dries clear.

Key features

  • Pre-Assembly Drying: Allow at least 5 minutes, or until tacky, before setting.
  • 30-Minute Bonding Window: Bonded surfaces should be assembled within 30 minutes of application.
  • Adjustable Spray Pattern: The nozzle provides low, medium, or high spray-width settings.

Applications

Headliners, carpets, trunk linings, door panels, and bonding foam, fabrics, plastics, and rubber.

Technical Specifications

General Properties
Chemistry Type
SIS Copolymer
Color
White
Other Properties
Storage Temperature
8 °C to 21 °C
Physical Properties
VOC
63.8 %

Leading Brands Trust in Our Products and Services