LOCTITE LB 8423
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- 19.8 kV/mm Dielectric Strength
- 2.6 x 10^15 ohm cm Resistivity
- -55 to 204 deg C Operating Range
Product Description
LOCTITE LB 8423 is a non-curing silicone dielectric compound supplied as a translucent thick paste for electrical connectors and lubricated interfaces. It is used on spark plug boots, distributor cap nipples, battery terminals, ignition-coil connectors, trailer electrical connectors, and on rubber, plastic, and ceramic surfaces. Typical application operating range is -55 to 204 deg C. Electrical properties include 19.8 kV/mm dielectric breakdown strength by IEC 60243-1, dielectric constant 3.0 with dissipation factor 0.007 at 1 kHz by IEC 60250, and volume resistivity of 2.6 x 10^15 ohm cm by IEC 60093.
Key features
- 19.8 kV/mm Dielectric Strength: Dielectric breakdown strength measured by IEC 60243-1.
- 2.6 x 10^15 ohm cm Resistivity: Volume resistivity measured by IEC 60093.
- -55 to 204 deg C Range: Typical application operating range is -55 to 204 deg C.
Applications
Spark plug boots, distributor cap nipples, battery terminals, ignition-coil connectors, trailer electrical connectors, and lubricated rubber, plastic, or ceramic interfaces.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Electrical Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Translucent paste | As supplied | |
| Specific gravity | 1.03 | 25 deg C | |
| Penetration | 250 | 1/10 mm | ISO 2137 |
In service
Non-curing grease; electrical values are bulk-compound measurements.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Operating range | -55 to 204 | deg C | Typical application range |
| Dielectric breakdown strength | 19.8 | kV/mm | IEC 60243-1 |
| Dielectric constant | 3.0 | IEC 60250, 1 kHz | |
| Dissipation factor | 0.007 | IEC 60250, 1 kHz | |
| Volume resistivity | 2.6 x 10^15 | ohm cm | IEC 60093 |