LOCTITE EA E-04SS

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA E-04SS

Main features

  • Very-Fast Cure for Short Cycles
  • Mixed-On-Demand Two-Part System
  • Metal Seam-Sealing Application

Product Description

LOCTITE EA E-04SS is a two-part epoxy adhesive system for fast seam sealing and metal bonding. Separate resin and hardener components are mixed before application, and the system uses a very fast cure profile for assembly processes where short handling times are important. The mixed epoxy is applied to seams or metal bonding areas and then cured as part of the assembly process. Applications include seam sealing and metal-to-metal bonding in industrial assembly operations.

Key features

  • Very fast cure: Rapid epoxy cure profile supports short-cycle seam-sealing assembly.
  • Two-part mixing: Separate resin and hardener are combined immediately before use.
  • Metal Seam Sealing and Bonding: Used for seam sealing and bonding metal assemblies.

Applications

Applications include seam sealing and metal-to-metal bonding in industrial assembly operations.

Technical Specifications

General Properties
Appearance
Epoxy: light gray | Hardener: Amber
Specific Gravity
Epoxy: 1.15 | Hardener: 1.13
Physical Properties
Viscosity
Epoxy: paste | Hardener: 2500 mPa.s
Thermal Properties
Flash Point
Epoxy: >93°C | Hardener: >93 °C