LOCTITE DRI 513HV

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE DRI513HV

Main features

  • High-Temperature Thread Sealing
  • Re-Adjustable Threaded Assemblies
  • Dry-Film Non-Curing Seal

Product Description

LOCTITE DRI 513HV is a one-part acrylic thread sealant that dries to a resilient, tight-clinging, non-curing seal on tapered or straight threaded plastic and metal pipes and fittings. It is designed for sealing and locking threaded assemblies that may require re-adjustment after installation. Typical use temperature is -20 to 150 deg C, with intermittent exposure up to 177 deg C. The high-viscosity liquid dries to a seal for threaded fittings, sensors, connectors and related assemblies where leak resistance and adjustability are important.

Key features

  • Non-curing thread seal: Dries to a resilient, tight-clinging seal on tapered or straight threads.
  • Thread-Seal Temperature Range: Typical use range is -20 to 150 deg C, with intermittent exposure up to 177 deg C.
  • Re-adjustable assemblies: Designed for threaded fittings where sealing and later re-adjustment are required.

Applications

Sealing and locking tapered or straight threaded plastic and metal pipes and fittings, including re-adjustment applications and common threaded fittings, sensors and connectors.

Technical Specifications

General Properties
Appearance
White liquid
Chemistry Type
Acrylic
Solids
54 to 72 %
Specific Gravity
1.02 to 1.18
Physical Properties
Viscosity
16,200 to 44,000 mPa.s
Other Properties
Storage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
Specific gravity1.02 to 1.1825 deg C; LMS
Viscosity16,200 to 44,000mPa sBrookfield RVT; spindle 6; 10 rpm; 25 deg C; LMS
pH7.0 to 8.025 deg C; LMS
Solids content54 to 72%LMS
On-part life4yearsStored in a cool, dry area
Technical properties

Final-state properties

PropertyValueUnitMethod / condition
Typical operating temperature-20 to 150deg CDocumented typical use range
Intermittent temperatureUp to 177deg CDocumented intermittent exposure
Heat-aged sealingPassed 1,035kPa3/8 in malleable iron NPT; 1 min leak test after documented heat aging
Automotive-fluid sealingNo leakage12.7 mm malleable iron NPT; 30-day immersion in listed automotive fluids; 1,035 kPa for 1 min