LOCTITE A-534R

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

LOCTITE A-534R

Main features

  • No-Drying-Time Cure Activation
  • Very Low-Viscosity Application
  • Fast Toughened-Acrylic Fixture Response

Product Description

LOCTITE SF A-534R is a red, solvent-free acrylic activator used to initiate cure of compatible LOCTITE toughened acrylic adhesives. The one-component, 100% solids liquid has very low viscosity and can be sprayed, wiped, or brushed as a thin film on a mating surface. No drying period is required before assembly. With LOCTITE A-533 on degreased steel using single-side activation, fixture is 30 seconds or less. Cure response depends on the adhesive and substrate used.

Key features

  • No-drying-time activation: Parts can be assembled immediately after the activator is applied.
  • Very low-viscosity liquid: Brookfield RVF viscosity is 50 mPa s (cP) maximum at 25 deg C with spindle 1 at 20 rpm.
  • Fast A-533 fixture response: Single-side activation on degreased steel fixtures LOCTITE A-533 in 30 seconds or less under ISO 4587 conditions.

Applications

Accelerating cure of compatible toughened acrylic adhesives.

Technical Specifications

General Properties
Appearance
Red
Chemistry Type
Acrylic
Specific Gravity
0.98
Physical Properties
Viscosity
≤50 mPa.s
Other Properties
Storage Temperature
2 °C to 8 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceRedAs supplied
Solids content100%As supplied
Specific gravity0.9825 deg C
Brookfield viscosity50 maximummPa s (cP)25 deg C; RVF; spindle 1; 20 rpm
Optimal storage temperature2 to 8deg CUnopened container in a dry location

Leading Brands Trust in Our Products and Services