LOCTITE 7380
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Solvent-Free Toughened Acrylic Activation
- Up to 6-Hour Active Window
- Fast LOCTITE 330 Fixture Development
Product Description
LOCTITE SF 7380 is a solvent-free, low-viscosity substituted dihydropyridine activator that initiates the cure of LOCTITE toughened acrylic adhesives. It is applied to one or both mating surfaces rather than mixed directly with the adhesive. The activator remains active for up to 6 hours, providing an assembly window after surface treatment. In an ISO 4587 test with LOCTITE 330 on grit-blasted steel and single-side activation, fixture time is up to 4 minutes. It is used with LOCTITE 330, 332, 334 and 392 toughened acrylic adhesives.
Key features
- Solvent-free activation: Transparent low-viscosity activator with no solvent.
- Extended active window: Treated surfaces remain active for up to 6 hours before assembly.
- Activator-assisted fixture time: Fixture time is up to 4 minutes with LOCTITE 330 on grit-blasted steel using single-side activation under ISO 4587.
Applications
Initiating cure of LOCTITE toughened acrylic adhesives, including 330, 332, 334 and 392.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 0.97 | 25 deg C | |
| Viscosity | 35 to 50 | mPa s | 25 deg C |
| Solvent | None | As supplied | |
| Optimal storage temperature | 8 to 21 | deg C | Unopened container; dry location; protect translucent containers from light |