LOCTITE 5182
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Controlled Continuous-Bead Dispensing
- Medium-Strength Flange Sealing
- Up to 0.5 mm Gasket Replacement
Product Description
LOCTITE 5182 is a one-part, red methacrylate ester gel for sealing close-fitting metal flange assemblies. Anaerobic cure begins under confinement between the mating surfaces, and the medium-strength, thixotropic material limits migration after application. Its gel form supports controlled continuous-bead dispensing, while the cured sealant is suited to housings, cases, and covers. It can replace cut gaskets up to 0.5 mm thick and can coat hard or soft cut gaskets to improve sealing performance. Flanges should be assembled and tightened promptly after application to avoid shimming.
Key features
- Thixotropic gel control: The red, high-viscosity gel limits migration after application.
- Close-fitting flange cure: Anaerobic cure develops between confined metal surfaces.
- Cut-gasket replacement and dressing: Replaces cut gaskets up to 0.5 mm thick or coats existing hard and soft gaskets.
Applications
Applications include gasketing and sealing housings, cases, and covers, plus repairing or replacing thin cut gaskets.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 1.1 | - | Typical at 25 deg C |
| Viscosity | 300,000 to 900,000 | mPa s (cP) | Specification range; Brookfield HBT, spindle TB, Helipath, 25 deg C, 0.5 rpm |
| Viscosity | 85,000 to 200,000 | mPa s (cP) | Specification range; Brookfield HBT, spindle TB, Helipath, 25 deg C, 5 rpm |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Coefficient of thermal expansion | 10 x 10^-4 | K^-1 | Typical; ISO 11359-2 |
| Thermal conductivity | 0.1 | W/(m K) | Typical; ISO 8302 |
| Specific heat | 0.3 | kJ/(kg K) | Typical |
| Compressive shear strength | >=5.5 | N/mm^2 | Specification minimum; ISO 10123, steel pins and collars, cured 1 hour at 22 deg C |
| Compressive shear strength | >=6.0 | N/mm^2 | Specification minimum; ISO 10123, steel pins and collars, cured 24 hours at 22 deg C |