LOCTITE 5144H is a high-viscosity ethyl cyanoacrylate adhesive formulated for bonding rubber substrates and other dissimilar or porous materials. This one-part, moisture-curing adhesive features a blue liquid appearance that supports visual quality control during application. Its viscosity helps accommodate small gaps, while its fast fixture speed on EPDM substrates can support efficient assembly processes. LOCTITE® 5144H™ develops functional bond strength rapidly and continues curing for up to 24 hours to achieve full chemical and solvent resistance.

Key features

  • High-viscosity formulation: Viscosity of 1,700–2,750 cP supports gap-filling applications and controlled dispensing.
  • Fast fixture speed: Achieves fixture time of ≤30 seconds on EPDM under test conditions.
  • Blue color for inspection: Facilitates visual quality verification during adhesive application.

Applications / Suitable for

  • Bonding EPDM and other rubber substrates
  • Joining dissimilar materials
  • Bonding porous materials
  • Assembly applications requiring rapid fixture times

Technical Specifications

General Properties
Appearance
Blue liquid
Chemistry Type
Ethyl cyanoacrylate
Physical Properties
Viscosity
1,700 to 2,750 mPa.s
Electrical Properties
Dielectric Strength
11.6 kV/mm
Other Properties
Storage Temperature
2 °C to 8 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the adhesive in its supplied state.

Property Value Unit Method / condition
Chemistry Ethyl cyanoacrylate — One-part adhesive
Appearance Blue liquid — Uncured state
Viscosity 1,700–2,750 cP 22°C, shear rate 100 s⁻¹
Fixture Time ≤30 seconds EPDM substrate
Storage Temperature 2–8 °C Recommended storage range
Technical properties

After-processing / final-state properties

Typical properties after 24 hours cure at 22°C.

Property Value Unit Method / condition
Tensile Strength 26 N/mm² ISO 6922, Aluminum-to-Aluminum
Softening Point 165 °C DIN EN 1427
Dielectric Breakdown Strength 11.6 kV/mm IEC 60243-1
Dielectric Constant 5.4 — IEC 60250, 1 kHz
Coefficient of Thermal Expansion 227 × 10⁻⁶ K⁻¹ 24-hour cure