LOCTITE 5127
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Vertical-Surface Gasketing Control
- No-Mix Anaerobic Flange Sealing
- Manual or Automated Dispensing
Product Description
LOCTITE 5127 is a one-part, blue methacrylate ester paste for form-in-place gasketing on close-fitting rigid metal flanges. The paste develops an anaerobic cure after confinement between mating metal surfaces, filling surface imperfections to form a tough, resilient seal. Its thixotropic consistency stays where applied on vertical surfaces and requires no mixing, with manual, screen-printing, roll-coating, and robotic-tracing application options. It can also repair damaged conventional gaskets or serve as a coating or dressing for them. Typical applications include pumps, housings, axle covers, gear cases, and split crankcases.
Key features
- Anaerobic flange cure: Cures between close-fitting metal flanges when confined in the absence of air.
- Thixotropic application control: The blue paste limits migration and can be applied on vertical surfaces.
- Manual and automated application: Can be applied by manual bead dispensing, screen printing, roll coating, or robotic tracing.
Applications
Applications include gasketing pumps, housings, axle covers, gear cases, and split crankcases, plus repairing or dressing conventional gaskets.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 1.1 | - | Typical at 25 deg C |
| Viscosity | 225,000 to 575,000 | mPa s (cP) | Specification range; Brookfield HBT, spindle TC, Helipath, 22 deg C, 0.5 rpm |
| Viscosity | 65,000 to 175,000 | mPa s (cP) | Specification range; Brookfield HBT, spindle TC, Helipath, 22 deg C, 5 rpm |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Elongation at break | 64 | % | Typical; ISO 527-3, cured 24 hours at 200 deg C |
| Tensile strength | 1.7 | N/mm^2 | Typical; ISO 527-3, cured 24 hours at 200 deg C |
| Lap shear strength | >=2 | N/mm^2 | Specification minimum; ISO 4587, steel, 0 gap, cured 24 hours at 22 deg C |
| Lap shear strength | 2.1 | N/mm^2 | Typical; ISO 4587, steel, 0.25 mm gap, cured 24 hours at 22 deg C |
| Lap shear strength | 1.2 | N/mm^2 | Typical; ISO 4587, aluminum, 0.25 mm gap, cured 24 hours at 22 deg C |
| Tensile strength | 0.8 | N/mm^2 | Typical; ISO 6922, steel pin to steel pin, cured 24 hours at 22 deg C |
| Peel strength | 0.85 | N/mm | Typical; ISO 8510-2, steel, 180 deg peel, cured 24 hours at 22 deg C |