LAIRD TPLI2110

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TPLI2110

Main features

  • Compliant 0.110-Inch Gap Filling
  • 6.0 W/(m K) Interface Conductivity
  • Electrically Insulating Thermal Path

Product Description

Tpli 2110 is a 0.110 in (2.75 mm) grade in Laird's Tpli 200 silicone thermal gap filler family. The boron nitride-filled sheet has a typical thermal conductivity of 6.0 W/(m K), Shore 00 hardness of 70, and density of 1.4 g/cc. Volume resistivity is 5 x 10^13 ohm cm, providing an electrically insulating interface material. Sheet size and adhesive configuration vary by part number, so the product represents the Tpli 2110 grade rather than one fixed cut part. It fills thermal interfaces in electronics across -45 to 200 deg C.

Key features

  • Grade thickness: The Tpli 2110 grade is 0.110 in (2.75 mm) thick.
  • Thermal conductivity: Typical thermal conductivity is 6.0 W/(m K) by ASTM D5470.
  • Electrical insulation: Typical volume resistivity is 5 x 10^13 ohm cm by ASTM D257.

Applications

Applications include automotive electronics, drones and satellites, gaming systems, notebooks and tablets, routers, smart-home devices, and wireless infrastructure.

Technical Specifications

General Properties
Density (g)
1.4 g/cm3
Thermal Properties
Temperature Range
-45°C to 200 °C
Thermal Conductivity
6.0 W/m.K
Electrical Properties
Volume Resistivity
5x10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Grade thickness is product-specific; remaining values are typical for the Tpli 200 family.

PropertyValueUnitMethod / condition
Grade thickness0.110in2.75 mm; configuration varies by part number
Thermal conductivity6.0W/(m K)Typical; ASTM D5470
Density1.4g/ccTypical; helium pycnometer
Hardness70Shore 00Typical; ASTM D2240
Volume resistivity5 x 10^13ohm cmTypical; ASTM D257
Temperature range-45 to 200deg CTpli 200 family range