LAIRD TFLEX P380

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX P380

Main features

  • Polyimide-Lined Electrical Isolation
  • 3.0 W/(m K) Thermal Conductivity
  • Pressure-Qualified Thermal Resistance

Product Description

Tflex P380 is a 0.080 in (2.03 mm) silicone gap filler with an integrated polyimide liner for thermal interfaces that also need handling strength and electrical isolation. The purple elastomer provides 3.0 W/(m K) thermal conductivity and Shore 00 hardness of 30. Exact-grade thermal resistance is 0.88 deg C in^2/W at 10 psi and decreases as pressure rises, giving designers pressure-specific performance data. The liner helps resist tearing and supports placement of the preformed sheet. A -40 to 125 deg C operating range, dielectric constant, volume resistivity, and breakdown-voltage data support electrical and thermal design screening.

Key features

  • Polyimide-lined construction: Integrated liner supports handling, placement, and electrical isolation.
  • 3.0 W/(m K) performance: Provides measured thermal conductivity for interface design.
  • Pressure-specific resistance: Exact-grade thermal resistance is published at 10, 30, and 50 psi.

Applications

Automotive ADAS; Automotive Electronics; Automotive Infotainment; Automotive Powertrain/ECUs; Drones/Satellites; Gaming Systems; Instrumentation; Notebooks/Tablets/Portable Devices; Routers; Smart Home Devices; Wireless infrastructure

Technical Specifications

General Properties
Color
Purple
Density (g)
3.10 g/cm3
Thermal Properties
Temperature Range
-40°C to 125 °C
Thermal Conductivity
3.0 W/m.K
Electrical Properties
Volume Resistivity
2×10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ConstructionPolyimide-lined silicone elastomerLaird Tflex P300 datasheet
Nominal thickness2.03 (0.080)mm (in)Exact Tflex P380 part page
ColorPurpleVisual
Density3.10g/ccHelium pycnometer
Hardness30Shore 00ASTM D2240
LinerIntegrated polyimideExact product family
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Thermal conductivity3.0W/(m K)ASTM D5470
Thermal resistance0.88deg C in^2/W10 psi; exact grade
Thermal resistance0.64deg C in^2/W30 psi; exact grade
Thermal resistance0.51deg C in^2/W50 psi; exact grade
Operating temperature range-40 to 125deg CLaird test
Dielectric constant4.601 MHz; ASTM D150
Volume resistivity2 x 10^14ohm-cmASTM D257
Breakdown voltage> 5kVASTM D149