LAIRD TFLEX HD760

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX HD760

Main features

  • Reduced Component-Load Conformance
  • 5.0 W/(m K) Heat Transfer
  • 0.060-Inch Gap-Filler Grade

Product Description

Tflex HD760 is a nominal 0.060 in high-deflection thermal gap filler from the Tflex HD700 series. The ceramic-filled silicone sheet pairs 5.0 W/(m K) thermal conductivity with low pressure-versus-deflection behavior, creating a conformable thermal interface that minimizes mechanical stress on boards and components. Its surface wetting lowers contact resistance, while typical family properties include 3.3 g/cm^3 density, Shore 00 hardness of 54, and a -50 to 200 deg C temperature range. This 60 mil grade serves thermal interfaces in automotive electronics, instrumentation, portable devices, routers, smart-home products, and wireless infrastructure.

Key features

  • 60 mil gap filler: Matches a nominal 0.060 in interface thickness.
  • Conformable heat path: Pairs low-pressure deflection with 5.0 W/(m K) conductivity.
  • Reduced interface stress: Limits mechanical loading on boards and components.

Applications

Automotive ADAS; automotive electronics; automotive infotainment; automotive powertrain/ECUs; drones and satellites; gaming systems; instrumentation; notebooks, tablets, and portable devices; routers; smart-home devices; wireless infrastructure.

Technical Specifications

General Properties
Color
Pink
Density (g)
3.3 g/cm3
Thermal Properties
Temperature Range
-50°C to 200 °C
Thermal Conductivity
2.7 W/m.K
Electrical Properties
Volume Resistivity
1.4x10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-Supplied Properties

Grade-specific nominal thickness; remaining values are typical for the Tflex HD700 material family.

PropertyValueUnitMethod / condition
Nominal thickness0.060inPart-number convention
Thickness tolerance+/- 10%Nominal
Construction and compositionCeramic-filled silicone sheetComposition
ColorPinkVisual
Density3.3g/cm^3Helium pycnometer
Hardness54Shore 00ASTM D2240
Technical properties

Installed Interface Properties

Typical Tflex HD700 material-family properties; thermal resistance is measured at 40 mil and 10 psi.

PropertyValueUnitMethod / condition
Thermal conductivity5.0W/(m K)ASTM D5470
Thermal resistance0.287deg C in^2/WASTM D5470 (modified); 40 mil, 10 psi
Temperature range-50 to 200deg CLaird test method
Dielectric constant5.01ASTM D150; 1 MHz
Volume resistivity1.4 x 10^14ohm-cmASTM D257
UL flammability ratingV-0UL 94