Main features

  • 5.0 W/(m K) Gap Bridging
  • Low-Stress Interface Compression
  • 0.100-Inch Thickness Selection

Product Description

Tflex HD7100 is the nominal 0.100 in thickness grade in the Tflex HD700 family of pink, ceramic-filled silicone thermal gap fillers. With 5.0 W/(m K) thermal conductivity and a thermal resistance of 0.287 deg C in^2/W at 40 mil and 10 psi, the material combines heat transfer with low pressure-versus-deflection behavior. Surface wetting lowers contact resistance, while the compliant interface minimizes stress on components. A Shore 00 hardness of 54 and a -50 to 200 deg C temperature range support evaluation for automotive electronics, drones and satellites, instrumentation, portable devices, routers, and wireless infrastructure.

Key features

  • 0.100 in gap coverage: Supplies a 100 mil Tflex HD700 thickness grade.
  • 5.0 W/(m K) conductivity: Creates a conductive thermal path across component gaps.
  • Low-pressure compliance: Reduces interface loading while maintaining surface contact.

Applications

Automotive ADAS; automotive electronics; automotive infotainment; automotive powertrain/ECUs; drones and satellites; gaming systems; instrumentation; notebooks, tablets, and portable devices; routers; smart-home devices; wireless infrastructure.

Technical Specifications

General Properties
Color
Pink
Density (g)
3.3 g/cm3
Thermal Properties
Temperature Range
-50°C to 200 °C
Thermal Conductivity
2.7 W/m.K
Electrical Properties
Volume Resistivity
1.4x10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-Supplied Properties

Grade-specific nominal thickness; remaining values are typical for the Tflex HD700 material family.

PropertyValueUnitMethod / condition
Nominal thickness0.100inPart-number convention
Thickness tolerance+/- 10%Nominal
Construction and compositionCeramic-filled silicone sheetComposition
ColorPinkVisual
Density3.3g/cm^3Helium pycnometer
Hardness54Shore 00ASTM D2240
Technical properties

Installed Interface Properties

Typical Tflex HD700 material-family properties; thermal resistance is measured at 40 mil and 10 psi.

PropertyValueUnitMethod / condition
Thermal conductivity5.0W/(m K)ASTM D5470
Thermal resistance0.287deg C in^2/WASTM D5470 (modified); 40 mil, 10 psi
Temperature range-50 to 200deg CLaird test method
Dielectric constant5.01ASTM D150; 1 MHz
Volume resistivity1.4 x 10^14ohm-cmASTM D257
UL flammability ratingV-0UL 94