LAIRD TFLEX B240
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- 0.040-Inch Preformed Gap Control
- 2 W/(m K) Interface Heat Transfer
- High-Resistivity Electrical Insulation
Product Description
Tflex B240 is the 0.040 in (1000 um) thickness grade in the ceramic-filled silicone Tflex B200 thermal gap-filler family. The compliant, low-modulus pad combines typical 2.0 W/(m K) thermal conductivity with natural tack on both sides for placement during assembly. Typical Shore 00 hardness is 42, and typical volume resistivity is 2 x 10^13 ohm cm. Standard, center-fiberglass MFG, and one-side FG configurations extend the family's handling options, while a -40 to 150 deg C temperature range supports electronic thermal-interface use.
Key features
- 1000-um thickness: 0.040 in (1000 um) preformed sheet.
- Thermal conductivity: Typical 2.0 W/(m K) conductivity carries heat across the interface.
- Electrical insulation: Typical volume resistivity is 2 x 10^13 ohm cm.
Applications
Applications include automotive ADAS, automotive infotainment, instrumentation, routers, and wireless infrastructure.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied properties
Typical Tflex B200 family data for the Tflex B240 thickness grade.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Construction | Ceramic-filled silicone sheet | - | Typical family construction |
| Nominal thickness | 0.040 (1000) | in (um) | Tflex B240 grade |
| Color | Gray | - | Visual |
| Density | 2.2 | g/cm^3 | Typical; helium pycnometer |
| Hardness | 42 | Shore 00 | Typical; ASTM D2240, 3-second reading |
Installed / in-service properties
Typical Tflex B200 family data for the Tflex B240 thickness grade. Thermal resistance is measured at 1.0 mm, not the nominal grade thickness.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Thermal conductivity | 2.0 | W/(m K) | Typical; ASTM D5470 |
| Thermal resistance | 1.10 | deg C in^2/W | ASTM D5470; 1.0 mm, 10 psi, 50 deg C |
| Temperature range | -40 to 150 | deg C | Laird test method |
| Volume resistivity | 2 x 10^13 | ohm cm | Typical; ASTM D257 |
| Flammability rating | V-0 | - | UL 94 |