LAIRD TFLEX 720

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX 720

Main features

  • 0.020-Inch Preformed Gap Control
  • 5 W/(m K) Interface Heat Transfer
  • Naturally Tacky Assembly Placement

Product Description

Tflex 720 is a 0.020 in (0.51 mm) silicone thermal gap-filler sheet in the Tflex 700 family. The dark gray, naturally tacky pad combines typical 5.0 W/(m K) thermal conductivity with a compliant interface that conforms to component topography. Its nominal thickness defines the 20-mil grade within the family's 0.020 to 0.200 in range. The material is electrically insulating and has an operating range of -40 to 200 deg C. Natural tack holds the pad during assembly and transport without an added adhesive coating.

Key features

  • 20-mil sheet: 0.020 in (0.51 mm) preformed thermal interface.
  • Thermal conductivity: Typical 5.0 W/(m K) conductivity supports interface heat transfer.
  • Assembly-ready surface: Natural tack holds the compliant pad during assembly and transport.

Applications

Applications include automotive electronics, instrumentation, routers, wireless infrastructure, and notebooks, tablets, and other portable devices.

Technical Specifications

General Properties
Color
Dark Grey
Density (g)
1.34 g/cm3
Specific Gravity
1.73
Thickness range
0.50 - 5.08 mm
Thermal Properties
Operating Temperature
-40°C to 200 °C
Temperature Range
-45°C to 200 °C
Thermal Conductivity
5.0 W/m.K
Electrical Properties
Volume Resistivity
2x10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied properties

Typical Tflex 700 family data for the Tflex 720 thickness grade.

PropertyValueUnitMethod / condition
ConstructionFilled silicone sheet-Typical family construction
Nominal thickness0.020 (0.51)in (mm)Tflex 720 grade
ColorDark gray-Visual
Density1.70g/cm^3Typical
Shelf life2yearsFrom date of shipment
Technical properties

Installed / in-service properties

Typical Tflex 700 family data for the Tflex 720 thickness grade.

PropertyValueUnitMethod / condition
Thermal conductivity5.0W/(m K)Typical; Hot Disk
Operating temperature-40 to 200deg CRange
Dielectric constant7.80-Typical
Volume resistivity1.00 x 10^13ohm cmTypical
Flammability ratingV-0-UL 94