LAIRD TFLEX 630

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX 630

Main features

  • Thin 0.030-Inch Gap-Filler Format
  • Compliant Low-Stress Interface Contact
  • Naturally Tacky Adhesive-Free Placement

Product Description

Tflex 630 has a nominal 0.030 in thickness within the Tflex 600 family, providing a thin ceramic-filled silicone gap-filler sheet for electronic thermal interfaces. Typical thermal conductivity is 3.0 W/(m K), with Shore 00 hardness of 51 and volume resistivity of 2 x 10^13 ohm cm. The highly compliant material is intended for low-stress contact and is naturally tacky, eliminating the need for an additional adhesive coating. It is electrically insulating and has a -45 to 200 deg C temperature range. Applications include automotive electronics, gaming systems, instrumentation, portable devices, routers, smart-home devices, and wireless infrastructure.

Key features

  • Thin 0.030 in format: The exact Tflex 600 grade provides a nominal 0.030 in sheet.
  • Compliant low-stress contact: Highly compliant construction is intended for low-stress thermal interfaces.
  • Natural assembly tack: The surface needs no additional adhesive coating for placement.

Applications

Automotive ADAS; automotive electronics; drones and satellites; gaming systems; instrumentation; notebooks, tablets, and portable devices; wireless infrastructure.

Technical Specifications

General Properties
Color
Blue-Violet
Density (g)
1.34 g/cm3
Thickness range
0.50 - 5.08 mm
Thermal Properties
Temperature Range
-45°C to 200 °C
Thermal Conductivity
3.0 W/m.K
Electrical Properties
Volume Resistivity
2x10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Tflex 630 is the nominal 0.030 in Tflex 600 grade; other values are typical for Tflex 600 material.

PropertyValueUnitMethod / condition
Construction and compositionCeramic-filled silicone sheet-As supplied
ColorBlue-violet-Visual; typical
Nominal thickness0.030inGrade code; thickness in mils
Hardness51Shore 00ASTM D2240; typical
Surface tackNaturally tacky on both sides-Standard construction; DC option changes tack configuration
ReinforcementFiberglass required-Required at 0.030 in thickness
Technical properties

After-processing / final-state properties

Typical Tflex 600 material data; thermal conductivity is a bulk value, not complete installed-interface performance.

PropertyValueUnitMethod / condition
Thermal conductivity3.0W/(m K)ASTM D5470; typical
Temperature range-45 to 200deg CTypical
Volume resistivity2 x 10^13ohm cmASTM D257; typical
Outgassing TML0.65%ASTM E595; typical
Outgassing CVCM0.21%ASTM E595; typical