LAIRD TFLEX 370TG

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX 370TG

Main features

  • Cut-Through-Resistant Tgard Barrier
  • Mass-Production Part Handling
  • Compliant 1.75 mm Gap Filling

Product Description

Tflex 370TG combines a 1.75 mm filled silicone thermal gap-filler sheet with a Tgard carrier liner. The reinforced construction supplies a cut-through-resistant dielectric barrier while improving part handling for mass production. Typical thermal conductivity is 1.2 W/(m K), Shore 00 hardness is 27 and nominal thickness tolerance is +/-10%. Low compression set permits repeated pad use, and the light-green material operates across -40 to 160 deg C. The sheet is adhesive on one side for placement.

Key features

  • Tgard dielectric barrier: Adds cut-through resistance to the reinforced sheet.
  • 1.75 mm grade thickness: Provides a preformed interface with +/-10% thickness tolerance.
  • Production handling: The carrier liner supports easier part handling in mass production.

Applications

Applications include telecom hardware, flat panels, memory modules, power conversion, automotive electronics, LED lighting and handheld electronics.

Technical Specifications

General Properties
Color
Light Green
Density (g)
1.80 g/cm3
Length
229 mm
Width
22.9 cm
Thermal Properties
Operating Temperature
-40 to 160 °C
Thermal Conductivity
1.20 W/m.K
Electrical Properties
Volume Resistivity
1.00 x10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Values describe the supplied preformed sheet before installation.

PropertyValueUnitMethod / condition
ConstructionFilled silicone elastomer on carrier linerTypical
Reinforcement carrierTgardExact family construction
ColorLight greenVisual
Nominal thickness1.75mmExact grade
Thickness tolerance+/-10%Typical
Specific gravity1.79ASTM D792
Hardness27Shore 00ASTM D2240
Shelf life2yearsFrom date of shipment
Technical properties

After-processing / final-state properties

Values describe bulk or compressed material under the stated test conditions, not complete assembly performance.

PropertyValueUnitMethod / condition
Thermal conductivity1.2W/(m K)ASTM D5470; typical
Thermal resistance1.59deg C in^2/WAt 10 psi; ASTM D5470 modified
Coefficient of thermal expansion600ppm/deg CIPC-TM-650 2.4.24
Operating temperature-40 to 160deg CTypical range
Breakdown voltageMore than 10,000VACASTM D149
Flammability rating94V0UL