LAIRD TFLEX 350

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX 350

Main features

  • 1.25 mm Gap-Filling Thickness
  • Compliant Low-Pressure Heat Transfer
  • Reusable Low-Compression-Set Pad

Product Description

Tflex 350 is a 1.25 mm ceramic-filled silicone sheet for compliant thermal gap filling in electronic assemblies. Typical thermal conductivity is 1.2 W/(m K), and the Tflex 300 material deflects more than 50% of its original thickness at 50 psi. A Shore 00 hardness of 25.2 for 40 mil and thicker material combines with low compression set for repeated placement. The light-green preformed pad has an operating temperature range of -40 to 160 deg C.

Key features

  • 1.25 mm preformed pad: Provides the exact thickness assigned to the 350 grade.
  • Conforming compression: More than 50% deflection at 50 psi promotes interface contact.
  • Reusable pad behavior: Low compression set allows repeated use.

Applications

Applications include automotive infotainment and electronics, gaming systems, instrumentation, notebooks and tablets, routers and wireless infrastructure.

Technical Specifications

General Properties
Color
Light Green
Density (g)
1.80 g/cm3
Length
457 mm
Width
45.7 cm
Thermal Properties
Operating Temperature
-40 to 160 °C
Thermal Conductivity
1.20 W/m.K
Electrical Properties
Volume Resistivity
1.00 x10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Values describe the supplied preformed sheet before installation.

PropertyValueUnitMethod / condition
Construction and compositionCeramic-filled silicone sheetTypical
ColorLight greenVisual
Nominal thickness1.25mmExact grade
Density1.78g/cm^3Helium pycnometer
Hardness25.2Shore 0040 mil and thicker; ASTM D2240
Shelf life2yearsFrom date of shipment
Technical properties

After-processing / final-state properties

Values describe bulk or compressed material under the stated test conditions, not complete assembly performance.

PropertyValueUnitMethod / condition
DeflectionMore than 50%At 50 psi; relative to original thickness
Thermal conductivity1.2W/(m K)ASTM D5470; typical
Operating temperature-40 to 160deg CTypical range
Dielectric constant4.5At 10 GHz; ASTM D150
Volume resistivity10^13ohm cmASTM D257