LAIRD LS-30/SS3
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- High-Loss LS-30 Microwave Grade
- Flexible Conductive Foam Construction
- SS3 Pressure-Sensitive Adhesive Backing
Product Description
Eccosorb LS-30/SS3 is a flexible polyurethane foam microwave absorber grade with an SS3 pressure-sensitive adhesive configuration. Carbon-black impregnation gives the foam its lossy, electrically conductive behavior for isolation, insertion loss, and cavity-resonance control above 1 GHz. Grade-level data for LS-30 include attenuation of 24 dB/cm at 3 GHz and 46 dB/cm at 10 GHz, with a maximum service temperature of 90 deg C. Multiple exact LS-30/SS3 thickness configurations are available for bonding to metal surfaces in RF amplifiers, oscillators, microwave cabinets, antenna-isolation structures, and other assemblies where reflection or surface-current reduction is needed.
Key features
- High-loss LS-30 grade: Typical attenuation is 24 dB/cm at 3 GHz and 46 dB/cm at 10 GHz.
- Flexible conductive foam: Carbon-black-impregnated polyurethane supports absorber placement on RF structures.
- SS3 adhesive configuration: Multiple exact LS-30/SS3 thickness configurations include pressure-sensitive adhesive.
Applications
RF amplifier and oscillator cavities, microwave-device cabinets, antenna isolation, reflection reduction, and surface-current control.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical LS-30 grade data with documented SS3 configuration scope; thickness-specific insertion loss is not generalized.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Material | Carbon-black-impregnated polyurethane foam | Eccosorb LS family | |
| Electrical behavior | Conductive | Carbon-black dispersion | |
| Frequency range | Above 1 | GHz | Typical family range |
| Maximum service temperature | 90 | deg C | Typical |
| Attenuation | 24 | dB/cm | LS-30; 3 GHz; typical |
| Attenuation | 46 | dB/cm | LS-30; 10 GHz; typical |
| Relative impedance | 0.13 / 0.22 | |Z|/Z0 | LS-30; 3 GHz / 10 GHz; typical |
| Backing | SS3 pressure-sensitive adhesive | Validated exact configurations |