LAIRD F2R2/PSA
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Fuel-Resistant Microwave Absorption
- Up-to-475-deg-F Temperature Capability
- PSA-Backed Aerospace Configurations
Product Description
F2R2/PSA is a fuel-resistant, fire-retardant fluorosilicone microwave absorber series with pressure-sensitive adhesive configurations for military and aerospace electronics. The F2R2 product line is engineered for equipment near jet engines and other harsh areas where absorber materials can encounter high heat, jet or missile fuel, fuel fumes, oils, and de-icing fluids. Manufacturer testing covers exposure to JP8 and JP10 fuels, oils, and de-icing fluids, and the absorber line can withstand temperatures up to 475 deg F. Exact PSA-backed thickness configurations support flight and cavity-resonance applications while keeping configuration-specific performance tied to the selected part.
Key features
- Fuel-resistant fluorosilicone absorber: The product line was tested with JP8 and JP10 fuels, oils, and de-icing fluids.
- High-temperature capability: F2R2 absorbers can withstand temperatures up to 475 deg F.
- Multiple PSA configurations: Pressure-sensitive adhesive versions are available in multiple exact thickness configurations.
Applications
Military and aerospace microwave absorption, production flight hardware, cavity-resonance control, and electronics near fuel and high-heat exposure.
Technical Specifications
Thermal Properties
Additional Information
As-supplied / before-processing properties
Product-line data for F2R2 with exact PSA configuration existence; thickness-specific performance is not generalized.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Material | Fluorosilicone | F2R2 product line | |
| Functional type | Fuel-resistant, fire-retardant microwave absorber | Product-line scope | |
| Backing | Pressure-sensitive adhesive | Validated exact configurations | |
| Temperature capability | Up to 475 | deg F | F2R2 absorber product line |
| Tested fluid exposure | JP8, JP10, oils, and de-icing fluids | Manufacturer product-line testing |