LAIRD COOLZORB-500
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Dual Thermal and EMI Management
- Broadband 1-to-90-GHz EMI Suppression
- Compliant Low-Stress Interface Contact
Product Description
CoolZorb 500 is a compliant hybrid thermal-interface and EMI-absorber sheet for placement between an IC or other heat source and a heat sink, heat-transfer device, or metal chassis. It combines 4.0 W/(m K) thermal conductivity with board-level EMI suppression across 1 to 90 GHz. Typical attenuation is 22.4 dB/cm at 10 GHz and 28.4 dB/cm at 20 GHz. Inherent surface tack supports placement, while Shore 00 59.5 hardness minimizes component stress during assembly. CoolZorb 500 provides simultaneous thermal transfer and suppression of unwanted coupling, resonances, and surface currents.
Key features
- Dual thermal and EMI control: The sheet combines 4.0 W/(m K) conductivity with EMI absorption.
- Broadband EMI suppression: EMI suppression spans 1 to 90 GHz.
- Compliant tacky interface: Inherent surface tack and Shore 00 59.5 hardness support assembly placement.
Applications
Thermal interfaces between ICs or other heat sources and heat sinks, heat-transfer devices, or metal chassis, with board-level EMI mitigation.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Values are typical product-selection data for the CoolZorb 500 series and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Thermal conductivity | 4.0 | W/(m K) | ASTM D5470; typical |
| Density | 3.5 | g/cm^3 | ASTM D792; typical |
| Hardness | 59.5 | Shore 00 | 3 sec; ASTM D2240; typical |
| Tensile strength | 17.3 | psi | ASTM D638; typical |
| Temperature range | -40 to 175 | deg C | Typical |
| Volume resistivity | 8 x 10^13 | ohm-cm | ASTM D257; typical |
| EMI attenuation | 22.4 | dB/cm | 10 GHz; typical |
| EMI attenuation | 28.4 | dB/cm | 20 GHz; typical |