INSULCURE 26

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

INSULCURE 26

Main features

  • Very-Large-Casting Epoxy Hardening
  • Extended 120-Minute Pot-Life Window
  • Low-Viscosity Material Handling

Product Description

Insulcure 26 is an epoxy curing agent for very large castings and good impact performance. Supplied viscosity is 800 cP at 25 deg C by ASTM D2393, while the 120-minute pot life provides a longer working window for casting preparation. The cure schedule is 36 hours at 25 deg C. Supplied as a single hardener product, Insulcure 26 is used with epoxy systems where extended processing time is required for large casting operations.

Key features

  • Very large casting use: The curing agent is intended for very large castings.
  • Extended pot life: Pot life is 120 minutes.
  • Low supplied viscosity: Viscosity is 800 cP at 25 deg C by ASTM D2393.

Applications

Epoxy curing and hardening for very large castings.

Product Family

INSULCURE 26

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Amber
Specific Gravity
0.94
Vapor Pressure
<1 mmHg
Thermal Properties
Boiling Point
> 160 °C
Flash Point
232.2 °C
Physical Properties
VOC
0

Additional Information

Technical properties

As-supplied / before-processing properties

Values are product-selection data for the curing agent and are not specifications.

PropertyValueUnitMethod / condition
Viscosity800cP25 deg C; ASTM D2393
Pot life120minCondition not stated
Cure schedule36h25 deg C