INSULCURE 20
Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations
Main features
- Low-Viscosity Epoxy Hardening
- 60-Minute Pot-Life Window
- Rapid Ambient-Temperature Cure
Product Description
Insulcure 20 is a low-viscosity epoxy curing agent for use as a hardener in epoxy systems. The supplied material has a viscosity of 700 cP at 25 deg C by ASTM D2393 and a 60-minute pot life. The cure schedule is 16 hours at 25 deg C. The product combines good impact performance with rapid cure, providing a fluid curing-agent option where a one-hour processing window is useful. As a standalone curing-agent product, it is intended for epoxy curing applications.
Key features
- Low supplied viscosity: Viscosity is 700 cP at 25 deg C by ASTM D2393.
- One-hour pot life: Pot life is 60 minutes.
- Rapid ambient cure: The cure schedule is 16 hours at 25 deg C.
Applications
Epoxy curing and hardening.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Values are product-selection data for the curing agent and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 700 | cP | 25 deg C; ASTM D2393 |
| Pot life | 60 | min | Condition not stated |
| Cure schedule | 16 | h | 25 deg C |