HUMISEAL 2A13

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

HUMISEAL 2A13

Main features

  • 1:1 Part A-to-Part B Mixing
  • 60-Minute Pot Life
  • Thermal Shock and Vibration Protection

Product Description

HumiSeal 2A13 is a two-component, low-stress polyurethane encapsulant for electronic sealing and encapsulation. It mixes at 1:1 and cures to a clear, elastic material used for electronic packages exposed to repeated thermal shock and high vibration. Typical component viscosities are 2,700 cP for Part A and 7,500 cP for Part B. Typical processing times are a 60-minute pot life, 120-minute handling time, and full cure after 24 hours at room temperature or one hour at 65 deg C. Substrates include metals, glass, ceramics, and plastics.

Key features

  • 1:1 Part A-to-Part B Mixing: Typical component viscosities are 2,700 cP for Part A and 7,500 cP for Part B.
  • 60-Minute Pot Life: Typical handling time is 120 minutes under the stated conditions.
  • Thermal Shock and Vibration Protection: The cured encapsulant is used for electronics exposed to repeated thermal shock and high vibration.

Applications

Electronic sealing and encapsulation on metals, glass, ceramics, and plastics.

Product Family

HUMISEAL 2A13

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
cloudy/clear (Part A/Part B)
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.00/1.95 (Part A/Part B)

Additional Information

Technical properties

As-supplied / before-processing properties

Typical two-component values from the 2018 HumiSeal Encapsulation Solutions brochure; time values may vary with volume or mix ratio.

PropertyValueUnitMethod / condition
ChemistryUrethane-Two-component system; manufacturer brochure
Part A viscosity2,700cPTypical component value
Part B viscosity7,500cPTypical component value
Mix ratio1:1-Part A:Part B; basis not stated
Pot life60minutesTypical 100 g volume
Handling time120minutesTypical 100 g volume
Technical properties

After-processing / final-state properties

Typical cured-system values from the 2018 HumiSeal brochure for the exact 2A13 configuration.

PropertyValueUnitMethod / condition
Full cure24 hours at RT or 1 hour at 65 deg C-Time may vary with volume or mix ratio
Cure typeTwo-component with heat option-Manufacturer brochure
ColorClear-Cured system
HardnessShore D31-Cured system
Operating temperature-50 to 110deg CCured system