HARDENER HW 5542
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- 2 to 3 Minute AW 5540 Work Life
- 1:1 AW 5540 Volume Mixing
- Automatic Mixing and Dispensing
Product Description
HARDENER HW 5542 is a standalone polyurethane adhesive hardener used in two Huntsman systems: ARALDITE AW 8680/HW 5542 and the legacy ARATHANE AW 5540/HW 5542. In the AW 5540/HW 5542 system, the red liquid hardener supports a 1:1 resin-to-hardener ratio by volume, a 2 to 3 minute work life at 25 deg C, and automatic mixing and dispensing. System-specific cure and performance values remain limited to the specific resin pairing in which they were measured.
Key features
- AW 5540 Work Life: The AW 5540/HW 5542 system has a 2 to 3 minute work life at 25 deg C.
- AW 5540 Volume Mixing: The system uses a 1:1 resin-to-hardener ratio by volume.
- Automatic Mixing and Dispensing: This processing method applies to the AW 5540/HW 5542 paired system rather than to the hardener alone.
Applications
Hardener component for polyurethane adhesive systems; the legacy AW 5540 pairing covers SMC, fiberglass-reinforced plastics, cured plastics, and metals.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical component values for HW 5542 from the exact manufacturer-authored AW 5540/HW 5542 system TDS.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Red liquid | - | HW 5542 hardener; visual |
| Specific gravity | 1.3 | - | HW 5542 hardener at 25 deg C; ASTM D792 |
| Viscosity | 20,000 | cP | HW 5542 hardener at 25 deg C; ASTM D2393 |