FREKOTE C-210

Harmonization Code : 3215907090 | Ink, whether or not concentrated or solid (excl. printing ink, printer/copier ink cartridges incorporating mechanical or electrical components, and solid ink in engineered shapes for printers/copiers)

FREKOTE C-210

Main features

  • Above 60 deg C Hot-Mold Touch-Up
  • Ready-to-Use No-Mix Emulsion
  • Spray, Brush, Wipe, or Dip

Product Description

LOCTITE FREKOTE C-210 is a water-based mold release product for hot-mold touch-up and spray application over a LOCTITE FREKOTE C-200 base coat. It is intended for touch-up on molds above 60 deg C or where spray application is used. The product is supplied ready to use, requires no mixing, and provides multiple releases without contaminating transfer to molded parts. It is a white emulsion with typical specific gravity of 1.00; application methods include spray, brush, wipe, or dip.

Key features

  • Hot-Mold Touch-Up: The product is intended for touch-up on molds above 60 deg C.
  • Ready-to-Use No-Mix Emulsion: The product is a white water-based emulsion with typical specific gravity of 1.00 and requires no mixing.
  • Spray, Brush, Wipe, or Dip: Spray is recommended for hot-mold touch-up; brush, wipe, and dip are alternative application methods.

Applications

Hot-mold touch-up; spray-applied mold release; use over a LOCTITE FREKOTE C-200 base coat.

Product Family

FREKOTE C-210

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White emulsion
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.00
Other Properties
Storage Temperature
Below 40 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical C-210 as-supplied values from the manufacturer-authored C-200/C-210 product description sheet.

PropertyValueUnitMethod / condition
AppearanceWhite emulsion-As supplied
OdorSlight mild-As supplied
Specific gravity1.00-Typical C-210 value
Storage limitBelow 40deg CSpecial caution in exact product sheet