EPOCAST 1645 FR
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- 1:1 Weight or Volume Mixing
- 2 to 3 Hour Sanding Window
- Aerospace Interior Flame Retardancy
Product Description
EPOCAST 1645 FR A/B is a two-component, ultra-low-density, flame-retardant epoxy void and edge filler for aerospace interior honeycomb structures. Both components are soft, non-sticky pastes that mix at 100:100 by weight or volume. The material can be applied manually, supports water cleanup after application, and is sandable within two to three hours. The room-temperature-curing system reaches a one-day cure and uses a color mix indicator for uniform blending. Applications include core reinforcement, edge sealing, component assembly, and aerospace interior honeycomb structures where FAR 25.853a and BMS 5-28 Type 9 requirements apply.
Key features
- 1:1 Weight or Volume Mixing: A color mix indicator provides a visual cue for uniform blending of Part A and Part B.
- 2 to 3 Hour Sanding Window: The system is sandable within this period and reaches a one-day cure at room temperature.
- Aerospace Interior Flame Retardancy: The system is used in interior honeycomb structures where FAR 25.853a requirements apply.
Applications
Aerospace interior honeycomb void filling; edge filling and sealing; core reinforcement; rapid component assembly.