ENTHONE IRIDITE 14-2

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE IRIDITE 14-2

Main features

  • Aluminum Alloy Conversion Coating
  • Corrosion-Resistance Function
  • Aerospace Finishing Process Use

Product Description

IRIDITE 14-2 is a chromate conversion-coating process for aluminum alloys used in aerospace finishing. It is used across multiple aerospace process specifications and provides corrosion resistance as a function of the treatment. Its application scope is aluminum conversion coating in aerospace finishing, with process selection and use governed by the applicable finishing specification and requirements for the target aluminum alloy.

Key features

  • Aluminum Conversion-Coating Process: IRIDITE 14-2 is used to treat aluminum alloys.
  • Corrosion-Resistance Function: The conversion coating provides corrosion resistance for treated aluminum alloys in the aerospace finishing context.
  • Aerospace Finishing Specification Use: Multiple aerospace process specifications use IRIDITE 14-2 for aluminum finishing.

Applications

Aluminum-alloy conversion coating; aerospace finishing.

Technical Specifications

General Properties
Color
Red
Density (g)
1.12 g/cm3