COOLTHERM SC-6715
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Multiple Hardener Pairing Options
- Automatic Meter-Mix-Dispense Application
- Dense-Component Potting Resin
Product Description
CoolTherm SC-6715 Silicone Resin is the resin component for two-component, solvent-free RTV silicone systems used in potting and encapsulation. As supplied, it is a white liquid with typical viscosity of 13,000 cP and specific gravity of 1.25 at 25 deg C. The resin is formulated for use with multiple CoolTherm hardeners, including SC-6730 and SC-6731. Those hardener choices provide different mix ratios and working-life schedules, and the mixed systems can be applied with automatic meter/mix/dispense equipment. Applications include potting densely packed components and producing flexible molds.
Key features
- Multiple Hardener Options: SC-6730 and SC-6731 are hardener options for use with SC-6715 resin.
- Automatic Meter/Mix/Dispense: The mixed silicone system can be applied with automatic meter/mix/dispense equipment.
- Potting and Mold Applications: Applications include potting densely packed components and producing flexible molds.
Applications
Resin component used with compatible CoolTherm hardeners for potting and encapsulating densely packed components and for producing flexible molds.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Electrical Properties
Thermal Properties
Mechanical Properties
Additional Information
As-Supplied Properties
Values apply to the SC-6715 resin component as supplied.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | White liquid | Typical; SC-6715 resin | |
| Viscosity | 13,000 | cP | Typical; SC-6715 resin; 25 deg C |
| Specific gravity | 1.25 | Typical; SC-6715 resin; 25 deg C |