CONAPOXY FR-1810

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CONAPOXY FR1810

Main features

  • Cartridge-Friendly 1:1 Mixing
  • Extended 80-Minute Work Life
  • High-Elongation Low-Stress Encapsulation

Product Description

CONAPOXY FR-1810 Epoxy Encapsulant is a two-component, filled, flame-retardant epoxy potting system for electronic components, modules, circuit boards and assemblies. Its 1:1 mix ratio by weight and volume accommodates cartridge, hand-mix and meter-mix processing. The mixed material has an initial viscosity of 8,000 cP at 25 deg C, an 80-minute work life for a 200 g mass, and a 36 deg C peak exotherm for a 225 g mass. After cure, the material combines 22% elongation with UL 94 V-0 performance at 4.8 mm.

Key features

  • Cartridge-Friendly 1:1 Mix: uses equal ratios by weight and volume for cartridge, hand-mix or meter-mix processing
  • 80-Minute Work Life: provides an 80-minute processing window for a 200 g mixed mass at 25 deg C
  • High-Elongation Cured Material: reaches 22% elongation under ASTM D412 at 25 deg C

Applications

Potting and encapsulation of electronic components, modules, circuit boards, assemblies and related electrical devices.

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
80 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for FR-1810 Part A, Part B and mixed material; the applicable state is identified by row.

PropertyValueUnitMethod / condition
Part A viscosity7,000cP25 deg C
Part B viscosity14,000cP25 deg C
Mix ratio100:100partsBy weight and by volume
Initial mixed viscosity8,000cP25 deg C
Work life80minutesTo 100,000 cP; 200 g mixed mass at 25 deg C
Gel time130minutes200 g mixed mass at 25 deg C
Peak exotherm36deg C225 g mixed mass at 25 deg C
Shelf life12monthsOriginal sealed containers; dry storage below 25 deg C, out of direct sunlight
Technical properties

After-processing / final-state properties

Values are typical for cured FR-1810 and are not specification limits.

PropertyValueUnitMethod / condition
Dielectric strength530V/milASTM D149 at 25 deg C; 1/16 inch specimen
Volume resistivity7.1 x 10^13ohm-cmASTM D257 at 25 deg C
Shore hardnessD 80ASTM D2240 at 25 deg C
Tensile strength1,300psiASTM D412 at 25 deg C
Elongation22%ASTM D412 at 25 deg C
Linear shrinkage0.06%ASTM D2566 at 25 deg C
Thermal conductivity0.7W/(m K)ASTM D5930
FlammabilityV-0UL 94 at 4.8 mm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers