BOSTIK SPA110

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

BOSTIK SPA110

Main features

  • 105 deg C Heat Activation
  • Dry Polyamide Web Lamination
  • Aerospace and Mobility Laminate Bonding

Product Description

Bostik SPA110 is a non-flame-retardant polyamide web adhesive used as a dry roll-form bonding layer in laminate constructions. The grade is heat activated at 105 deg C and provides a web-format alternative to liquid adhesive application for heated lamination processes. Its polyamide web construction is used in aerospace decorative-laminate bonding and in heated lamination of SMC/aluminum constructions for mobility and battery assemblies. The roll format supports controlled placement of adhesive across layered parts while keeping the bonding material in a dry, handleable web before activation.

Key features

  • 105 deg C Heat Activation: The SPA110 grade is identified with a 105 deg C activation temperature.
  • Dry Polyamide Web: Roll-form web provides a dry adhesive layer for heated lamination.
  • Laminate Construction Fit: Applications include aerospace decorative laminates and SMC/aluminum constructions.

Applications

Aerospace decorative-laminate bonding and heated lamination of SMC/aluminum constructions in mobility and battery assemblies.

Product Family

BOSTIK SPA110

Loading pricing…

Technical Specifications

No specifications available.