BOSTIK SH4275

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

BOSTIK SH4275

Main features

  • 20-71 g/m^2 Basis-Weight Options
  • Approx. 130 deg C Heat Activation
  • Industrial Filter and Textile Laminating

Product Description

Bostik Sharnet 4275 is an off-white nonwoven polyester web adhesive for industrial lamination. The web is configured in 20 to 71 g/m^2 basis weights and trimmed widths from 10 to 68 in, with a 120 deg C melt point and an approximately 130 deg C minimum activation temperature. Its dry nonwoven format provides a handleable adhesive layer for controlled laminate construction without liquid coating. Applications include industrial filter-media laminates, engineered laminates, and textile laminates, giving the grade a defined role in roll-based heat-activated bonding processes.

Key features

  • Defined Basis-Weight Range: The polyester web spans 20 to 71 g/m^2 basis weights for laminate construction.
  • Heat-Activated Web: Minimum activation temperature is approximately 130 deg C.
  • Industrial Laminate Applications: Uses include filter-media, engineered, and textile laminates.

Applications

Industrial filter-media laminates, engineered laminates, and textile laminates.

Product Family

BOSTIK SH4275

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Off-White nonwoven fabric
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
20-71 g/m2
Width
25 - 173 cm
Chemical Properties
Melting Point
120

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
AppearanceOff-white nonwovenAs supplied
Basis weight range20 to 71g/m^2Web basis-weight range
Trimmed width10 to 68inRoll web
Melt point120deg CAs supplied
Minimum activation temperatureApprox. 130deg CHeat activation