BOSTIK F14-588
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- High-Shear Heat-Resistant Film Bonding
- Plasticizer and Shrink Resistance
- Flexible Decorative Film Lamination
Product Description
Bostik F14-588 is a flame-retardant acrylic pressure-sensitive adhesive film for laminating flexible PVF and vinyl decorative materials in aircraft and mass-transit interiors. The configurable film is available in 2 mil and 3 mil thicknesses, with dry-film weights of approximately 60 and 90 g/m^2. It combines high shear strength with heat resistance, good creep and peel performance, and resistance to plasticizer migration and shrinkage. Serviceable bonds are identified from -20 to 160 deg F, and the moisture-stable liner is designed for controlled handling during decorative laminate fabrication.
Key features
- High shear and heat resistance: Combines strong shear performance with resistance to elevated service temperatures.
- Plasticizer and shrink resistance: Resists plasticizer migration and shrinkage in flexible decorative-film constructions.
- Two thickness formats: Available in 2 mil and 3 mil adhesive-film configurations.
Applications
Laminating flexible PVF and vinyl decorative films for aircraft and mass-transit interior constructions.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Film thickness | 2 and 3 | mil | Available configurations; TDS also gives 51 and 76 um |
| Dry film weight | about 60 and 90 | g/m^2 | Available film weights |
| Volatiles | <3.0 | % | As supplied |
| Release from paper liner | 12 | g/in | 6 mil paper liner; TDS also gives 4.7 g/cm |
| Release from LDPE liner | 40 | g/in | 4 mil LDPE liner; TDS also gives 16 g/cm |
| Shelf life | 12 | months | Stored dry at 40 to 80 deg F |